Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ULTEM™ Resin 1000P - PEI - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for ULTEM™ Resin 1000P:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultem datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
ULTEM 1000P Resin is an unreinforced amorphous polyetherimide (PEI) powder. This powder is available with an average particle size (D50) of 350 micron. It may offer a high glass transition temperature (Tg) of 217°C. Features are excellent mechanical, electrical and dimensional properties up to high temperatures. The material may offer very good chemical resistance for an amorphous material and is inherently flame retarded. The material is RoHS Compliant. The base material is transparent amber colored.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 13 cm³/10min ISO 1133
Temperatura 360 °C -
Carga 5 kg -
ASTM Data
Índice de fluidez, MFI 9 g/10min ASTM D 1238
Temperatura 337 °C -
Carga 6.6 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 3200 MPa ISO 527
Esfuerzo de fluencia 110 MPa ISO 527
Alarg. en límite elástico 6 % ISO 527
Alargamiento a rotura 50 % ISO 527
Modulo de Flexión 3300 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 4 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 4 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm N kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm N kJ/m² ISO 180/1U
Res. impacto Izod c/entalla, +23°C, 4mm 6 kJ/m² ISO 180/1A
Res. impacto Izod c/entalla, -30°C, 4mm 6 kJ/m² ISO 180/1A
Dureza Rockwell M 106 - ISO 2039-2
Ball indentation hardness 140 MPa ISO 2039-1
ASTM Data
Módulo de tracción 3350 MPa ASTM D 638
Esfuerzo de fluencia a tracción 115 MPa ASTM D 638
Alargamiento a la fluencia 7 % ASTM D 638
Alargamiento a la rotura 60 % ASTM D 638
Módulo de flexión 3200 MPa ASTM D 790
Dureza Rockwell M 109 - ASTM D 785
Resistencia a la abrasión (Taber) 10 mg/1000 cycles ASTM D 1044
Resistencia al impacto Izod con entalla, 1/8 in 53 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 50 J/m ASTM D 256
Temperatura -30 °C -
Resistencia al impacto Izod, 1/8 in 1800 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 192 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 209 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, A 215 °C ISO 306
Temp. reblandecimiento Vicat, B 211 °C ISO 306
Temp. reblandecimiento Vicat, 120°C/h 50N 212 °C ISO 306
Conductibilidad termica 0.22 W/(m K) DIN 52616
ASTM Data
Estabilidad al calor @ 66 psi 207 °C ASTM D 648
Estabilidad al calor @ 264 psi 190 °C ASTM D 648
Temperatura Vicat 211 °C ASTM D 1525
Conductividad térmica, estado sólido 0.0317 W/(m K) ASTM C 177
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 1MHz 2.9 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 60 E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 33 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 150 - IEC 60112
ASTM Data
Resistencia dieléctrica, tiempo corto 19.7 kV/mm ASTM D 149
Resistividad volumétrica >1E15 Ohm*cm ASTM D 257
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 1.25 % Sim. to ISO 62
Densidad 1270 kg/m³ ISO 1183
Densidad 1270 kg/m³ ASTM D 792
Características
Características especiales
Transparente
Resistencia quimica
Resistencia química general
Certifications
RoHS
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.