Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Sarlink® 4775B42 - TPV - Teknor Apex Co.

Material Data Center offers the following functions for Sarlink® 4775B42:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sarlink datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

The Sarlink TPV 4700 Series are very high flow injection molding engineering grades with excellent UV resistance, elasticity, and surface aesthetics designed for demanding automotive applications including window encapsulation and exterior parts. Sarlink TPV 4775B42 is a black, medium hardness, low density thermoplastic vulcanizate suited for injection molding applications that require superior flow properties.



PropertyValueUnitStandard
Tensile properties (Cross Flow Direction)

ISO 37
   Tensile strength at break      6,3 MPa
   Modulus at 100% elongation      3,2 MPa
   Elongation at break    470 %
Hot air aging (168h/150°C, Cross Flow Direction)

ISO 188
   Change in hardness        1 points
   Change in tensile strength at break     -19 %
   Change in modulus at 100% elongation        2 %
   Change in elongation at break     -24 %
Hot air aging (1000h/135°C, Cross Flow Direction)

ISO 188
   Change in hardness      -2 points
   Change in tensile strength at break    -18 %
   Change in modulus at 100% elongation       3
%
   Change in elongation at break    -28
%
Volume swell (70h/125°C in IRM 903 oil)     73 % ISO 1817
Apparent shear viscosity @ 206 1/s, 200°C    200 Pa.s ISO 11443 Capillary
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Deformación permanente por compresión a 23°C, 24h 24 % ISO 815
Deformación permanente por compresión a 70°C, 24h 39 % ISO 815
Dureza Shore A 76 - ISO 7619-1
Other Standards[S]
Tensión a 100% alargamiento 3.4 MPa ISO 37
Resistencia a la tracción TPE 5.8 MPa ISO 37
Alargamiento a rotura TPE 410 % ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 910 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Negro
Características especiales
Estable contra rayos U.V./interperie
Resistencia quimica
Resistencia química general
Applicaciones
Automotriz, Encapsulacion
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.