Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PPcompound 8620A - PP - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PPcompound 8620A:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, high stiffness, and cold temperature ductility is required. IMDS ID: 209747752
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Índice de fluidez, MFI 12 g/10min ISO 1133
Temperatura 230 °C -
Carga 2.16 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1660 MPa ISO 527
Esfuerzo de fluencia 17 MPa ISO 527
Alarg. en límite elástico 3.8 % ISO 527
Resistencia a la tracción 13 MPa ISO 527
Alargamiento a rotura 41 % ISO 527
Módulo de flexión, 23°C 1780 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 55 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 6 kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla 6 kJ/m² ISO 180/1A
ASTM Data
Módulo de tracción 1890 MPa ASTM D 638
Esfuerzo de fluencia a tracción 17 MPa ASTM D 638
Esfuerzo de fractura a tracción 12 MPa ASTM D 638
Alargamiento a la fluencia 4.7 % ASTM D 638
Alargamiento a la rotura 101 % ASTM D 638
Módulo de flexión 1420 MPa ASTM D 790
Dureza D Shore 54 - ASTM D 2240
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 56 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 100 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, A 122 °C ISO 306
ASTM Data
Estabilidad al calor @ 66 psi 99 °C ASTM D 648
Estabilidad al calor @ 264 psi 53 °C ASTM D 648
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1030 kg/m³ ISO 1183
Densidad 1030 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 - 100 °C -
Tiempo de pre-secado 2 - 4 h -
Temperatura de la masa 210 - 270 °C -
Temperatura del molde 15 - 60 °C -
Zona 1 190 - 230 °C -
Zona 2 200 - 250 °C -
Zona 3 210 - 270 °C -
Temperatura de boquilla 210 - 270 °C -
Contrapresión 1 - 1.5 MPa -
Características
Características especiales
Alto impacto o modificado al impacto
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.