Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Panlite® LV-2225Y - PC - Teijin Chemicals Ltd.

Material Data Center offers the following functions for Panlite® LV-2225Y:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Panlite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 11 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
ASTM Data
Contracción posterior al moldeo, paralelo 0.006 mm/mm ASTM D 955
Contracción posterior al moldeo, normal 0.006 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2400 MPa ISO 527
Esfuerzo de fluencia 61 MPa ISO 527
Alarg. en límite elástico 6 % ISO 527
Alarg. nominal a rotura >50 % ISO 527
Módulo de flexión, 23°C 2350 MPa ISO 178
Resistencia a la flexión 92 MPa ISO 178
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 71 kJ/m² ISO 179/1eA
ASTM Data
Módulo de tracción 2130 MPa ASTM D 638
Esfuerzo de fluencia a tracción 62 MPa ASTM D 638
Esfuerzo de fractura a tracción 78 MPa ASTM D 638
Alargamiento a la fluencia 6 % ASTM D 638
Alargamiento a la rotura 140 % ASTM D 638
Resistencia de compresión 76 MPa ASTM D 695
Módulo de flexión 2260 MPa ASTM D 790
Resistencia a la flexión 90 MPa ASTM D 790
Dureza Rockwell M 77 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 830 J/m ASTM D 256
Resistencia al impacto Izod con entalla, 1/4 in 130 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 128 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 141 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 148 °C ISO 306
Coef.de expansión térmica lineal, paralelo 70 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 70 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. V-2 class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Combustibilidad a espesor h V-2 class IEC 60695-11-10
Espesores de probeta 0.4 mm -
Glow Wire Flammability Index (GWFI) 825 °C IEC 60695-2-12
GWFI - thickness tested (1) 1.5 mm -
Glow Wire Flammability Index (GWFI) 875 °C IEC 60695-2-12
GWFI - thickness tested (2) 3.2 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (2) 3.2 mm -
ASTM Data
Combustibilidad UL 94 V-2 - UL 94
Espesores de probeta 3 mm -
Coeficiente de dilatación térmica, long. 70 E-6/K ASTM D 696
Coeficiente de dilatación térmica, normal 70 E-6/K ASTM D 696
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 3.1 - IEC 62631-2-1
Constante dieléctrica, 1MHz 3 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 10 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 90 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 30 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 250 - IEC 60112
ASTM Data
Resistencia dieléctrica, tiempo corto 30 kV/mm ASTM D 149
Factor de pérdidas dieléctricas, 60 Hz 0.0004 - ASTM D 150
Factor de pérdidas dieléctricas, 1 MHz 0.009 - ASTM D 150
Constante dieléctrica, 60 Hz 2.95 - ASTM D 150
Constante dieléctrica, 1 MHz 2.9 - ASTM D 150
Resistividad volumétrica 3E16 Ohm*cm ASTM D 257
Resistencia al arco 110 s ASTM D 495
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Transmitancia luminosa 88 % ASTM D 1003
Índice de refracción 1.58 - ASTM D 542
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1200 kg/m³ ISO 1183
Absorción de agua, equilibrio 0.2 % ASTM D 570
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 120 °C -
Tiempo de pre-secado >5 h -
Temperatura de la masa 270 - 320 °C -
Temperatura del molde 80 - 120 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Aditivos
Desmoldeante
Características especiales
Transparente
Applicaciones
Uso general
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.