Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin LS6010 - Americas - (PPE+PS) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin LS6010 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
NORYL™ LS6010 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This high performance, injection moldable and extrudable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0 at 1.5mm. NORYL LS6010 resin features low smoke production upon burning, high heat resistance, very low specific gravity, enhanced resistance to melting and dripping and meets the requirements of FAR 25.853. In addition, this material is heat stabilized and impact modified. It is an excellent candidate for aerospace interior applications such as rub strips, seat track covers, cable guides, switch panels, conduit, wall/ceiling mounted electronics, and parts machined from slab stock.

UL Yellow Card Link E121562-644041
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 5 cm³/10min ISO 1133
Temperatura 280 °C -
Carga 5 kg -
ASTM Data
Índice de fluidez, MFI 5.6 g/10min ASTM D 1238
Temperatura 280 °C -
Carga 5 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2440 MPa ISO 527
Esfuerzo de fluencia 64 MPa ISO 527
Alarg. en límite elástico 4.7 % ISO 527
Resistencia a la tracción 58 MPa ISO 527
Alargamiento a rotura 8.3 % ISO 527
Modulo de Flexión 2360 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 20 kJ/m² ISO 179/1eA
Res. impacto Izod c/entalla, +23°C, 4mm 18 kJ/m² ISO 180/1A
Res. impacto Izod c/entalla, -30°C, 4mm 14 kJ/m² ISO 180/1A
ASTM Data
Módulo de tracción 2220 MPa ASTM D 638
Esfuerzo de fluencia a tracción 64 MPa ASTM D 638
Esfuerzo de fractura a tracción 53 MPa ASTM D 638
Alargamiento a la fluencia 4.6 % ASTM D 638
Alargamiento a la rotura 20 % ASTM D 638
Módulo de flexión 2390 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 300 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 181 J/m ASTM D 256
Temperatura -30 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 124 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 143 °C ISO 306
Temp. reblandecimiento Vicat, 120°C/h 50N 146 °C ISO 306
Combustibilidad a 1.5mm esp. nom. V-0 class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
Estabilidad al calor @ 264 psi 122 °C ASTM D 648
Temperatura Vicat 143 °C ASTM D 1525
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.2 % Sim. to ISO 62
Absorción de humedad 0.05 % Sim. to ISO 62
Densidad 1110 kg/m³ ISO 1183
Densidad 1110 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 95 - 105 °C -
Tiempo de pre-secado 2 - 4 h -
Temperatura de la masa 280 - 305 °C -
Temperatura del molde 65 - 100 °C -
Zona 1 280 - 295 °C -
Zona 2 290 - 300 °C -
Zona 3 295 - 305 °C -
Velocidad de giro de husillo 40 - 80 rpm -
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusión de perfiles, Extrusión de láminas
Aditivos
Ignifugante
Características especiales
Resistencia mejorada al fuego, Alto impacto o modificado al impacto
Applicaciones
Automotriz
Disponibilidad regional
Norteamérica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.