Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer EXL8414 - Americas - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer EXL8414 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
LEXAN EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are longer due to limited manufacturing capability. Higher color variability and contamination risks including black specs needs to be considered before approval for use in applications. Contact your technical sales representative with questions.

UL Yellow Card Link E121562-100150790
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 8 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
ASTM Data
Índice de fluidez, MFI 9.2 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2360 MPa ISO 527
Esfuerzo de fluencia 57 MPa ISO 527
Alarg. en límite elástico 6 % ISO 527
Resistencia a la tracción 58 MPa ISO 527
Alargamiento a rotura 50 % ISO 527
Modulo de Flexión 2170 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 82 kJ/m² ISO 179/1eA
Res. impacto Izod c/entalla, +23°C, 4mm 67 kJ/m² ISO 180/1A
Res. impacto Izod c/entalla, -30°C, 4mm 56 kJ/m² ISO 180/1A
ASTM Data
Módulo de tracción 2150 MPa ASTM D 638
Esfuerzo de fluencia a tracción 57 MPa ASTM D 638
Esfuerzo de fractura a tracción 60 MPa ASTM D 638
Alargamiento a la fluencia 6 % ASTM D 638
Alargamiento a la rotura 113 % ASTM D 638
Módulo de flexión 2210 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 852 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 741 J/m ASTM D 256
Temperatura -30 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. reblandecimiento Vicat, B 143 °C ISO 306
Temp. reblandecimiento Vicat, 120°C/h 50N 145 °C ISO 306
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Glow Wire Flammability Index (GWFI) 825 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
Estabilidad al calor @ 66 psi 138 °C ASTM D 648
Estabilidad al calor @ 264 psi 126 °C ASTM D 648
Temperatura Vicat 143 °C ASTM D 1525
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.35 % Sim. to ISO 62
Absorción de humedad 0.15 % Sim. to ISO 62
Densidad 1190 kg/m³ ISO 1183
Densidad 1180 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 120 °C -
Tiempo de pre-secado 3 - 4 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 295 - 315 °C -
Temperatura del molde 70 - 95 °C -
Zona 1 270 - 295 °C -
Zona 2 280 - 305 °C -
Zona 3 295 - 315 °C -
Velocidad de giro de husillo 40 - 70 rpm -
Contrapresión 0.3 - 0.7 MPa -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Certifications
Contenido de resina reciclada
Disponibilidad regional
Norteamérica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.