Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin NH5020 - Asia - (PPE+PS) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin NH5020 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
NORYL™ NH5020 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and exhibits high heat resistance with thin-wall FR performance. NORYL NH5020 resin carries a UL94 flame rating of V0 at 0.75mm along with a UL746C Outdoor Suitability rating of F1. The material offers a good balance of affordable high heat, flow, hydrolytic stability, excellent creep resistance, dimensional stability and is a good candidate for photovoltaic / solar connectors, UPS Inverters / chargers, and outdoor enclosure applications.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 10 cm³/10min ISO 1133
Temperature 280 °C -
Load 5 kg -
Density of melt 1010 kg/m³ -
Thermal conductivity of melt 0.2 W/(m K) -
Spec. heat capacity of melt 1780 J/(kg K) -
Ejection temperature 127 °C -
ASTM Data
Melt Flow Index, MFI 9.8 g/10min ASTM D 1238
Temperature 280 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3050 MPa ISO 527
Yield stress 80 MPa ISO 527
Yield strain 4.7 % ISO 527
Stress at break 77 MPa ISO 527
Strain at break 5.6 % ISO 527
Flexural modulus 2980 MPa ISO 178
Charpy notched impact strength, +23°C 7 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C, 4mm 8 kJ/m² ISO 180/1A
Izod notched impact strength, -30°C, 4mm 6 kJ/m² ISO 180/1A
ASTM Data
Tensile Modulus 2720 MPa ASTM D 638
Tensile Strength at Yield 79 MPa ASTM D 638
Tensile Strength at Break 62 MPa ASTM D 638
Elongation at Yield 5 % ASTM D 638
Elongation at Break 15 % ASTM D 638
Flexural Modulus 3000 MPa ASTM D 790
Izod Impact notched, 1/8 in 91 J/m ASTM D 256
Izod Impact notched, Low-Temperature 59 J/m ASTM D 256
Temperature -30 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 119 °C ISO 75-1/-2
Vicat softening temperature, B 138 °C ISO 306
Vicat softening temperature, 120°C/h 50N 139 °C ISO 306
Coeff. of linear therm. expansion, parallel 83.8 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 85.8 E-6/K ISO 11359-1/-2
ASTM Data
DTUL @ 66 psi 122 °C ASTM D 648
DTUL @ 264 psi 117 °C ASTM D 648
Vicat Temperature 137 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Water absorption 0.25 % Sim. to ISO 62
Humidity absorption 0.05 % Sim. to ISO 62
Density 1110 kg/m³ ISO 1183
Density 1110 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 105 - 110 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 275 - 305 °C -
Mold temperature 70 - 100 °C -
Zone 1 245 - 295 °C -
Zone 2 255 - 300 °C -
Zone 3 265 - 305 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 0.7 MPa -
Diagrams
Viscosity-shear rate , NORYL™ Resin NH5020 - Asia, (PPE+PS), SABIC
Shearstress-shear rate , NORYL™ Resin NH5020 - Asia, (PPE+PS), SABIC
Specific volume-temperature (pvT) , NORYL™ Resin NH5020 - Asia, (PPE+PS), SABIC
Characteristics
Processing
Injection Molding
Additives
Flame retarding agent
Special Characteristics
Flame retardant
Chemical Resistance
Hydrolytically Stable
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.