Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grilamid TR 90 natural - PAMACM12 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grilamid TR 90 natural:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Grilamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Product-nomenclature: ISO 16396-PAMACM12,,GT,C14-020

 

Transparent Polyamide

Product Attributes

  Highly transparent

Markets

  Automotive
  Automotive electr. and electronics, lighting, Cooling and climate control, Fuel systems,
Powertrain and Chassis, Interior
  Electricals & Electronics
  Electrical appliances, Electrical equipment, Connectors, Energy distribution,
Mobile phones and other portable devices, Lighting
  Industry & Consumer goods
  Heating systems, Housewares, Hydraulics & Pneumatics, Mechanical Engineering, Medical devices,
Power transmission, Sanitary, water and gas supply, Sports & Leisure, Tools & Accessories
  Optics
  Lenses, Optical components, Safety glasses, Sunglasses, Spectacle frames
  Packaging
  Non oriented film, Cosmetics / Personal care, Medical packaging

Approvals

  Food Contact
  EU Requirements, FDA
  Medical
  USP VI, ISO 10993
  Potable Water Contact
  NSF 61, KTW, WRAS, DVGW W270
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.7 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.8 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 1600 / 1600 MPa ISO 527
Yield stress 60 / 60 MPa ISO 527
Yield strain 7 / 6 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 13 / 13 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 12 / 12 kJ/m² ISO 179/1eA
Shore D hardness 81 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min 155 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 115 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 135 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 90 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 90 / * E-6/K ISO 11359-1/-2
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity 1E11 / 1E11 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E12 Ohm IEC 62631-3-2
Electric strength 34 / 34 kV/mm IEC 60243-1
Comparative tracking index - / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 3 / * % Sim. to ISO 62
Humidity absorption 1.5 / * % Sim. to ISO 62
Density 1000 / - kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Grilamid TR 90 natural, PAMACM12, EMS-GRIVORY
Shearstress-shear rate , Grilamid TR 90 natural, PAMACM12, EMS-GRIVORY
Dynamic Shear modulus-temperature , Grilamid TR 90 natural (cond.), PAMACM12, EMS-GRIVORY
Stress-strain , Grilamid TR 90 natural (cond.), PAMACM12, EMS-GRIVORY
Secant modulus-strain , Grilamid TR 90 natural (cond.), PAMACM12, EMS-GRIVORY
Stress-Strain (Film Grades) , Grilamid TR 90 natural (cond.), PAMACM12, EMS-GRIVORY
Stress-strain (isochronous) 23°C, Grilamid TR 90 natural (cond.), PAMACM12, EMS-GRIVORY
Creep modulus-time 23°C, Grilamid TR 90 natural (cond.), PAMACM12, EMS-GRIVORY
Creep curve 23°C, Grilamid TR 90 natural (cond.), PAMACM12, EMS-GRIVORY
Specific volume-temperature (pvT) , Grilamid TR 90 natural, PAMACM12, EMS-GRIVORY
Tensile modulus-temperature , Grilamid TR 90 natural (cond.), PAMACM12, EMS-GRIVORY
Fatigue strength , Grilamid TR 90 natural, PAMACM12, EMS-GRIVORY
Characteristics
Processing
Injection Molding, Other Extrusion
Delivery form
Granules, Natural Color
Special Characteristics
Transparent
Certifications
Food contact, Food approval FDA 21 CFR, Drinking water contact, Drinking water contact KTW, Drinking water contact DVGW W270, Drinking water contact NSF 61, Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
Applications
Automotive, Electrical and Electronical, Medical, Packaging, Sports Equipment
Regional Availability
Other text information
Other extrusion
-- PIPE EXTRUSION --
-- SHEATING --
PROCESSING
Melt temperature : 250-270 °C
Feeding bush : 60-90
Barrel temp. profile : 240-250 °C
Head temp. : 250-240 °C

Please consider the information about the application of the materials.
Chemical Media Resistance
Acids
Acetic Acid (5% by mass) (23°C)
Citric Acid solution (10% by mass) (23°C)
Lactic Acid (10% by mass) (23°C)
Hydrochloric Acid (36% by mass) (23°C)
Nitric Acid (40% by mass) (23°C)
Sulfuric Acid (38% by mass) (23°C)
Sulfuric Acid (5% by mass) (23°C)
Chromic Acid solution (40% by mass) (23°C)
Bases
Sodium Hydroxide solution (35% by mass) (23°C)
Sodium Hydroxide solution (1% by mass) (23°C)
Ammonium Hydroxide solution (10% by mass) (23°C)
Alcohols
Isopropyl alcohol (23°C)
Methanol (23°C)
Ethanol (23°C)
Hydrocarbons
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Ketones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Mineral oils
SAE 10W40 multigrade motor oil (23°C)
SAE 10W40 multigrade motor oil (130°C)
SAE 80/90 hypoid-gear oil (130°C)
Insulating Oil (23°C)
Standard Fuels
ISO 1817 Liquid 1 (60°C)
ISO 1817 Liquid 2 (60°C)
ISO 1817 Liquid 3 (60°C)
ISO 1817 Liquid 4 (60°C)
Standard fuel without alcohol (pref. ISO 1817 Liquid C) (23°C)
Standard fuel with alcohol (pref. ISO 1817 Liquid 4) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (90°C)
Diesel fuel (pref. ISO 1817 Liquid F) (>90°C)
Salt solutions
Sodium Chloride solution (10% by mass) (23°C)
Sodium Hypochlorite solution (10% by mass) (23°C)
Sodium Carbonate solution (20% by mass) (23°C)
Sodium Carbonate solution (2% by mass) (23°C)
Zinc Chloride solution (50% by mass) (23°C)
Other
Ethyl Acetate (23°C)
Hydrogen peroxide (23°C)
DOT No. 4 Brake fluid (130°C)
Ethylene Glycol (50% by mass) in water (108°C)
1% nonylphenoxy-polyethyleneoxy ethanol in water (23°C)
50% Oleic acid + 50% Olive Oil (23°C)
Water (23°C)
Deionized water (90°C)
Phenol solution (5% by mass) (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.