Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Zylar® 631 - MBS - INEOS Styrolution

Material Data Center offers the following functions for Zylar® 631:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Zylar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 5 g/10min ISO 1133
Temperature 200 °C -
Load 5 kg -
ASTM Data
Melt Flow Index, MFI 5 g/10min ASTM D 1238
Temperature 200 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2140 MPa ISO 527
Yield stress 36 MPa ISO 527
Flexural modulus, 23°C 2050 MPa ISO 178
Flexural strength 61 MPa ISO 178
ASTM Data
Tensile Modulus 2137 MPa ASTM D 638
Tensile Strength at Yield 35.9 MPa ASTM D 638
Elongation at Break 40 % ASTM D 638
Flexural Modulus 2068 MPa ASTM D 790
Flexural Strength 60.7 MPa ASTM D 790
Rockwell Hardness R 70 - ASTM D 785
Izod Impact notched, 1/8 in 117 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Vicat softening temperature, A 99 °C ISO 306
ASTM Data
UL 94 Flame rating HB - UL 94
Vicat Temperature 99.4 °C ASTM D 1525
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1.5 % ASTM D 1003
Light Transmittance 89 % ASTM D 1003
Index of Refraction 1.56 - ASTM D 542
Other propertiesValueUnitTest Standard
Water absorption 0.1 % Sim. to ISO 62
Density 1050 kg/m³ ISO 1183
Water Absorption, Equilibrium 0.1 % ASTM D 570
Density 1050 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 65.6 °C -
Pre-drying - Time 2 h -
Melt temperature 204 - 238 °C -
Mold temperature 26.7 - 54.4 °C -
Zone 1 179 - 213 °C -
Zone 2 185 - 218 °C -
Zone 3 191 - 224 °C -
Characteristics
Processing
Injection Molding
Special Characteristics
High impact or impact modified, Transparent, Sterilizable, Ethylene Oxide (EtO) Sterilization, Gamma irradiation sterilization
Features
Copolymer
Chemical Resistance
Radiation Resistance
Certifications
Medical Grade, US Pharmacopeia Class VI Approved
Applications
Medical, Packaging
Regional Availability
North America, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.