Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PA11 ESD - PA11 - BASF

Material Data Center offers the following functions for Ultrasint PA11 ESD:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 20 / * cm³/10min ISO 1133
Temperature 220 / * °C -
Load 2.16 / * kg -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 204 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 111 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 186 / * °C ISO 75-1/-2
Vicat softening temperature, A 192 / * °C ISO 306
Vicat softening temperature, B 183 / * °C ISO 306
Other propertiesdry / condUnitTest Standard
Density 1070 / - kg/m³ ISO 1183
Bulk density 460 kg/m³ -
3D Datadry / condUnitTest Standard
Other Standards[S]
Tensile modulus, flat 3150 / 2300 MPa ISO 527
Tensile modulus, upright 2150 / 1550 MPa ISO 527
Tensile strength, flat 65 / 55 MPa ISO 527
Tensile strength, upright 55 / 47 MPa ISO 527
Strain at break, flat 20 / 22 % ISO 527
Strain at break, upright 23 / 31 % ISO 527
Flexural modulus, flat 3050 / 2550 MPa ISO 178
Flexural modulus, upright 2100 / 1650 MPa ISO 178
Charpy impact strength, +23°C, flat 80 / 101 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, upright 90 / 107 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C, flat 6.6 / 7.3 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, upright 4.7 / 5.3 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, flat 67 / 81 kJ/m² ISO 180/1U
Izod impact strength, +23°C, upright 58 / 83 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, flat 7 / 7.9 kJ/m² ISO 180/1A
Izod notched impact strength, +23°C, upright 5 / 5.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Additive Manufacturing, Laser Sintering
Delivery form
Powder
Chemical Resistance
General Chemical Resistance
Certifications
Contains renewable resources
Applications
Electrical and Electronical
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.