Material datasheets available free. Online registration at: www.materialdatacenter.com
Tinuvin - UV-light stabilizers - BASF SE
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Tinuvin" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...rt. With the development of light stabilisers (LS) by Ciba Specialty Chemicals and the choice of a suitable flame-retardant system, polypropylenes (PP) now have an extended lifetime in outdoor applications. The flame-retardant stabiliser system TinuvinFR (manufacturer: Ciba Specialty Chemicals) is suitable for long-life PP applications, such as stadium seating (title photo, Fig.1), transport boxes, profiles, structural parts and clothing elements of all kinds. This product can meet a wide range ...
Kunststoffe international, 2005-11-21, Flame Retardants: Growing Demand
...in the company's range include the oligomeric phosphates PFR 500, 600 and 700, designed for engineering plastics and blends. Ciba Specialty Chemicals presented two new flame-retardant systems with a particularly high light stability – Tinuvin FR 2011 and 2021. These were developed especially for polypropylene in outdoor applications, such as seat shells in stadiums. Other products in the company's flame-retardant range are melamine derivatives and light stabilisers used as flame-retarda...
Kunststoffe international, 2005-11-21, HALS Light Stabiliser: Light Stabilisation and More
... different temperatures (light stabilisers from other suppliers mentioned in the text: HALS 1: Chimassorb 944 from Ciba Speciality Chemicals, Basel/Switzerland; HALS 2: Hostavin N 30 from Clariant International, Muttenz/Switzerland; HALS 3: Tinuvin 622 from Ciba Speciality Chemicals, Basel; HALS 4: Uvasil HA 88 from 3V Sigma, Bergamo/Italy) Manufacturer BASF AG G-EVP/PP – J 550 D-67056 Ludwigshafen Germany Phone +49 (0) 6 21/60-44021 Fax +49 (0) 6 21/60-6644021 www.basf.de/lightstabilizers
Kunststoffe international, 2005-11-21, Integrated Solutions
...on of paint to partially painted bumpers. It proved necessary to develop innovative light stabilisers in order to solve this problem. Slightly alkaline products were seen to be advantageous in this specific application. The high-performance Tinuvin XT 850 system was thus developed, which can also be used under critical conditions. This ensures excellent light stabilisation even at low concentrations. This effect is particularly noticeable in moulded-in-colour polyolefins (Table2). Stringent requ...
Kunststoffe international, 2005-11-21, Stabilization - Doping for Recyclates
...esistance-oriented restabilization, the variant with 1 % Recycloblend 660 was used as the basis for the heat ageing trials. To make the PP regrind mixture suitable for outdoor applications, it was mixed with, among other things, various amounts of Tinuvin 791. Fig. 5 illustrates the influence of the weathering-oriented restabilization compared with non-restabilized mixtures and the reference virgin material. Without UV stabilization, a clearly visible discolouration of the surface occurs after o...
Kunststoffe international, 2006-05-23, Innovative Potential: Additives Now and in the Future
...es. For example, Ciba Specialty Chemicals Ltd. in Basel/Switzerland has launched the following products for special fields of application over the last few years: - light stabiliser to impart excellent stability to plasticised PVC [8] (grade: Ciba Tinuvin XT 833), - light stabiliser for agricultural films in contact with pesticides [9] (grade: Ciba Tinuvin NOR 371), - long-term weathering resistance of pigmented TPO exterior automotive parts [10] (grade: Ciba Tinuvin XT 850), - multifunctional s...
Kunststoffe international, 2010-08-19, Profitable and Faster than the Market
... color strength, heat resistance as well as colorfastness in outdoor applications. A long product life even when exposed to strong sunlight is ensured by the lightstabilizing additives from the Chimassorb and Tinuvin families that were initially developed by Ciba and are now part of BASF. According to Reiners, with this integrated approach, not only is the additives product range strengthened; the previous Ciba business within the unit has also gained in importance significantly from the new, mo...
Kunststoffe international, 2010-09-24, A Motley Range of Innovations
...us innovations is impressive. BASF Extensive Range Following the acquisition of Swissbased Ciba in 2010, BASF SE, Ludwigshafen, Germany, is the market leader in the field of additives and pigments. A new addition to its range of light stabilizers is Tinuvin XT 200, a UV absorber for use in greenhouse films. The additive is characterized by a very high resistance to sulfur and agricultural chemicals, which is a practical requirement for a very long service life. For PE-LD film, for example, this ...
Kunststoffe international, 2013-04-19, Automatic Corrections and Calculations
...ties which affect the dispersion of the pigment. In order to illustrate this in the following trial the content of additives was varied widely. For example changing the concentration of the stabilizer (grade: Tinuvin 622 and Irganox 1010, manufacturer: BASF SE, Ludwigshafen, Germany) by just 0.1 % resulted in a color deviation of 1.11 and 0.82 respectively in a polypropylene (PP) compound (grade: Sabic PP 505P, manufacturer: Sabic ...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.