Material datasheets available free. Online registration at: www.materialdatacenter.com
Tencel - C - Lenzing Plastics GmbH
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Tencel" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
... sustainable fiber that would solve this problem. The mechanical properties of natural fibers often depend on factors such as climate, harvest conditions or weak points due to growth anomalies. The raw material of Tencel FCP (Fibrous Cellulose Powder) is wood, which is converted into a cellulosic fiber in an environment-friendly process. Through this process, all limiting factors of natural fibers are eliminated. Tencel FCP is produced from pure cellulose, this increases the thermal stability of...
Kunststoffe international, 2014-11-26, Low Weight and Sustainability for Vehicles
...in terms of long-term and UV stability, too. The Development Goes OnApart from optimizing matrix material and phasing, crucial improvements to the fibers may also be possible. Special cellulose regenerate fibers such as, most of all, the Tencel microfiber by Lenzing AG in Lenzing, Austria, include the option to further enhance the potentials of NPP properties and applications. On a PP homopolymer basis, this group of materials can yield the highest performance in terms of impact resistance as w...
Kunststoffe international, 2018-02-21, Keeping Track of Elongation
...Fig. 6, right) reveals clear differences in terms of type as well as the fiber filling content. The fiber compounds were produced using a low-flow polypropylene (type: PP HB 600 TF, producer: Borealis) and cellulose fibers (type: Tencel, producer: Lenzing AG, Lenzing, Austria), plus conventional chopped glass fibers.Application Possibilities for the Extrusion RheometerThe application examples clearly illustrate that the novel online elongation and shear rheometer represents a useful further dev...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.