Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin CN5260 - Asia - (PPE+PS)-(MX+GF)50 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin CN5260 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
NORYL CN5260 resin is a 50% mineral and glass fiber reinforced blend of polyphenylene ether (PPE) + polystyrene (PS). This high modulus, injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VB at 2mm and V1 at 1.5mm. NORYL CN5260 resin exhibits good dimensional stability, low moisture absorption, and high rigidity. It is an excellent candidate for printer chassis applications.

UL Yellow Card Link: E207780-228542
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 13.3 g/10min ASTM D 1238
Temperature 300 °C -
Load 5 kg -
Mold Shrinkage, MD 0.002 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Flexural Modulus 12350 MPa ASTM D 790
Flexural Strength 161 MPa ASTM D 790
Izod Impact notched, 1/8 in 58 J/m ASTM D 256
Other Standards[S]
Tensile Strength at Yield 129 MPa Producer Method
Elongation at Break 5 % Producer Method
S: These properties are reported by the producer according standards that are different to our defaults.
Thermal propertiesValueUnitTest Standard
ISO Data
Burning behav. at 1.5 mm nom. thickn. V-1 class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Burning behav. 5V at thickness h 5VB class IEC 60695-11-20
Thickness tested 2.0 mm -
Yellow Card available yes - -
ASTM Data
UL 94 Flame rating V-1 - UL 94
Thickness tested 1.5 mm -
DTUL @ 264 psi 125 °C ASTM D 648
Other propertiesValueUnitTest Standard
Water Absorption, 24hr 0.06 % ASTM D 570
Density 1530 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 100 °C -
Pre-drying - Time 3 - 4 h -
Melt temperature 280 - 300 °C -
Mold temperature 70 - 90 °C -
Zone 1 260 - 280 °C -
Zone 2 270 - 290 °C -
Zone 3 280 - 300 °C -
Nozzle temperature 280 - 300 °C -
Back pressure 0.5 - 1.2 MPa -
Characteristics
Processing
Injection Molding
Additives
Flame retarding agent
Special Characteristics
Flame retardant, Halogen-free
Applications
IT / Business Machine, Electrical and Electronical
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.