![Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.](/rev13959/modules/../customized/tradenames/views/images/seo_en.png)
Material datasheets available free. Online registration at: www.materialdatacenter.com
Nordel - EPDM - The Dow Chemical Company
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Nordel" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
... is used with Saret SR-522 coagent (Sartomer, Exton, PA/USA), a diacrylate ester, for applications such as radiator hoses. Similar trends can be seen with other manufacturers’ products, for example Nordel 1040 (HD grade from DPPE). DPPE has added to its Nordel MG range of metallocene gas phase products. These grades have ethylene contents from 50 to 80% and Mooney viscosities from 60 to 200 and complement the IP grades and conventional EPDM grades. Nordel MG delivers a 5 to 10% increased mixer f...
Kunststoffe international, 2005-11-21, Elastomers
... a new oil-extended EPDM with a well-balanced microstructure, which is claimed to permit high heating rates and excellent extrudability, even for extremely difficult profiles. The Nordel IP grades unveiled by DuPont Dow Elastomers (DDE) at K’98 were complemented at K’01 with Nordel MG metallocene gas-phase grades, which are produced by the process originally presented by Union Carbide [3] in 1995. With ethylene contents of 50 to 80% and Mooney viscosities from 60 to 200, they provide a complemen...
Kunststoffe international, 2005-11-21, Plastic, the All-purpose Material: Function in Form
...lass-fibre-reinforced polyarylamide PAMXD6 GF50 (grade: IXEF1022; Fig.3) [4]. The tyre manufacturer Cheng Shin Rubber Industry Co. Ltd., Taiwan, makes bicycle inner tubes and tyres from a hydrocarbon rubber (grade: Nordel-IP) from DuPont Dow Elastomers. The tyre treads and flanks are made of a Nordel MG blended with natural rubber (NR) and styrene-butadiene rubber (SBR). The tyres and inner tubes now improve the severe demands that mountain bike races, such as the “Maxxis International Cup” make...
Kunststoffe international, 2005-11-21, Tailored EPDM
... With the introduction of single-site catalysts with fixed geometry (CGC), a new class of polyolefin elastomers was born [1, 2, 3]. Following the success of Engage ethylene-octene copolymers, and the completion of DuPont Dow Elastomer's range of Nordel IP EPDM polymers, further ethylene copolymers based on metallocene technology are now poised for market launch. Nordel IP is the first mass-produced EPDM based on this catalyst. For the first time it is possible to selectively control the mole...
Kunststoffe international, 2007-01-22, Extended Product Range
...tion with plastics processors and OEMs in the development of innovative products. Gudrun Klein The distributor and compounder Resin Express GmbH of Zwingenberg/Germany has now extended its portfolio to include Versify plastomers and elastomers and Nordel EPDM rubbers from Dow, polyolefin specialities from Borealis for the automotive industry, and Enflex-V TPE-V and Ensoft-S SEBS/polyolefin compounds from Enplast. From Highly Elastic to Supersoft Versify is a new group of versatile polypropyl...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.