Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Monprene® CP-18250 - TPE - Teknor Apex Co.
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Monprene datasheets, application examples or technical articles are available in Material Data Center
The Monprene CP-18200 Unfilled, High Flow Series of thermoplastic elastomer compounds, with good UV resistance, available in NAT or colors, from 40 to 80 Shore A, are designed specifically for EU consumer product applications requiring a soft, rubber-like feel. Monprene CP-18250 is a medium hardness, low density grade that is suitable for injection molding.
Adheres to PP
Property | Value | Unit | Standard |
---|---|---|---|
Apparent Viscosity (200 °C, 206 1/s) | 99 | Pas | ASTM D3835 |
Mechanical properties | Value | Unit | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Compression set at 23 °C, 24h | 24 | % | ISO 815 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Compression set at 70 °C, 24h | 44 | % | ISO 815 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ASTM Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Modulus at 100% Elongation | 1.4 | MPa | ASTM D 412 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Modulus at 300% Elongation | 0.67 | MPa | ASTM D 412 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Shore A Hardness | 50 | - | ASTM D 2240 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Tensile Strength at Break | 7.5 | MPa | ASTM D 412 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Elongation at Break | 800 | % | ASTM D 412 |
Other properties | Value | Unit | Test Standard |
Density | 890 | kg/m³ | ASTM D 792 |
Processing Recommendation Injection Molding | Value | Unit | Test Standard |
Pre-drying - Temperature | 65 | °C | - |
Pre-drying - Time | 2 - 4 | h | - |
Melt temperature | 180 - 230 | °C | - |
Mold temperature | 15 - 50 | °C | - |
Zone 1 | 120 - 160 | °C | - |
Zone 2 | 160 - 230 | °C | - |
Zone 3 | 180 - 230 | °C | - |
Nozzle temperature | 180 - 230 | °C | - |
Screw speed | 50 - 100 | rpm | - |
Back pressure | 0.5 - 1.5 | MPa | - |
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.