Any use of this information falls under the rules of our
disclaimer.
Processing/Physical Characteristics | Value | Unit | Test Standard |
Other Standards[S] |
Molding shrinkage, parallel |
0.1 |
% |
DIN 16901 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Tensile Modulus |
15000 |
MPa |
ISO 527 |
Tensile Strength |
170 |
MPa |
ISO 527 |
Charpy impact strength, +23°C |
47 |
kJ/m² |
ISO 179/1eU |
Thermal properties | Value | Unit | Test Standard |
ISO Data |
Temp. of deflection under load, 1.80 MPa |
240 |
°C |
ISO 75-1/-2 |
Other Standards[S] |
Coeff. of linear therm. expansion, parallel |
4 |
E-6/K |
DIN 53752 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Electrical properties | Value | Unit | Test Standard |
ISO Data |
Surface resistivity |
100 |
Ohm |
IEC 62631-3-2 |
Other properties | Value | Unit | Test Standard |
Density |
1400 |
kg/m³ |
ISO 1183 |
Processing Recommendation Extrusion | Value | Unit | Test Standard |
Pre-drying - Temperature |
130 |
°C |
- |
Pre-drying - Time |
6 - 8 |
h |
- |
Melt temperature |
280 |
°C |
- |
Zone 1 |
260 - 300 |
°C |
- |
Zone 2 |
260 - 300 |
°C |
- |
Zone 3 |
260 - 300 |
°C |
- |
Nozzle temperature |
250 - 290 |
°C |
- |
Characteristics
Processing
Other Extrusion, Additive Manufacturing
Delivery form
Pellets, Black, Natural Color
Special Characteristics
Heat stabilized or stable to heat
Applications
Automotive, Filament for 3D Printing
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.