Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Hostacom G3 R05 105555 - PP-GF30 - LyondellBasell Industries

Material Data Center offers the following functions for Hostacom G3 R05 105555:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Hostacom datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Hostacom G3 R05 105555 is a 30% glass fiber reinforced PP homopolymer, with excellent stiffness, good dimensional stability and low creep under load at elevated temperatures. The product is available in black color, pellet form. This grade is delivered in 105555 color version.

This material is able to replace Polyamide glass filled compounds especially in structural applications. 
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 4 cm³/10min ISO 1133
Temperature 230 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 7100 MPa ISO 527
Stress at break 98 MPa ISO 527
Strain at break 3 % ISO 527
Charpy impact strength, +23°C 50 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 11 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 8 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 168 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 145 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 160 °C ISO 75-1/-2
Vicat softening temperature, B 135 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 3.0 mm -
Burning rate, FMVSS, Thickness 1 mm 40 mm/min ISO 3795 (FMVSS 302)
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Other propertiesValueUnitTest Standard
Density 1140 kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Delivery form
Granules, Black
Special Characteristics
Heat stabilized or stable to heat
Features
Creep Resistance, Homopolymer
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Application examples
Battery box
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com