Material datasheets available free. Online registration at: www.materialdatacenter.com
Flamestab - Flame retardants, UV-light stabilizers - BASF SE
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Flamestab" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...atives. Surprisingly, it was then found that certain nitroxyl ethers (NOR-HALS) work synergistically to improve flame retardancy and can be effective, even on their own, without another flame retardant. Ciba Specialty Chemicals Ltd. developed Ciba Flamestab NOR 116 (Fig.2), a very effective, multifunctional flame retardant for polypropylene fibres and films (Fig.3), which – because of its chemical structure – also helps impart light stability and long-term heat resistance [15]. The activity of N...
Kunststoffe international, 2011-04-25, Flame Retardants: Restricted Boom
...00 and 800 are organic nitrogen and phosphorus compounds, while TL 1260, which is just being introduced to the market, is a pure phosphorus-based substance. They are effective alone or synergistically with sterically hindered amines such as Flamestab NOR 116 (BASF, Ludwigshafen, Germany) or Hostavin NOW (Clariant International Ltd., Muttenz, Switzerland). In LDPE films, Class B2 according to DIN 4102 or Euroclass E is achieved with 4 to 8 % PCO 700 or 6 to 8 % PCO 800. When these products are us...
Kunststoffe international, 2014-08-19, Eco-Friendly Fire Prevention
...pyrophosphoric acid salt available under the name Zuran 808.3 (Chitec Technologies, supplied by Raimund Müller GmbH & Co KG, Prisdorf, Germany).In 1999, Ciba Specialty Chemicals (now BASF SE) introduced a revolutionary flame retardant known as Flamestab NOR 116 (Fig. 5) for polypropylene and polyolefins in the form of films and fibers [15]. Its effect is based on very rapid polymer degradation in a fire, as a result of which the polymer retreats from the flame. As a compound based on sterically ...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.