Material datasheets available free. Online registration at: www.materialdatacenter.com
Elvax - EVAC - DuPont Packaging & Industrial Polymers
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Elvax" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...alogen-free – replacement of PCV in the construction sector and other applications. These new ethylene-acrylate copolymers extend DuPont’s portfolio of special ethylene copolymers for polymer modification, which also includes Elvax ethylene-vinyl acetate (EVA) and Fusabond maleic anhydride (MAH)-grafted polyolefins, Surlyn ionically crosslinked plastics, SelarPA amorphous polyamides and ElvaloyHP and PTW ethylene-acrylate terpolymers with polar CO or epoxy functionality. The Authors of this Ar...
Kunststoffe international, 2007-05-14, Big Opportunity for the Plastics Industry
...eat-resistant and can be laminated at high temperatures. Materials for the Encapsulation of Solar Cells To encapsulate solar cells, DuPont provides three different materials adapted to a large variety of solar panel applications. Elvax EVA has been available at the market for more than 25 years. Sheets made of this material have favourable optical properties, low gel content as well as high polarity, and their properties remain the same for a long time. What is more, they can easily be process...
Kunststoffe international, 2014-06-17, Some Ways Lead to Rome, but Some Do Not
...oiling, dust and other particles (Fig. 5). The two moldings must therefore close easily in all openings, and require little power for drawing off the sealing mat.The sealing mat is produced from an EVA material in a single-cavity mold (type: Elvax; manufacturer: DuPont), while the well plate is made of PP (type: Purell; manufacturer: Lyondell Basell) in a two-cavity mold. In both cases, a critical aspect is to safeguard homogenous filling of the moldings as well as constant filling times. In th...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.