Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® RA100CPE NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® RA100CPE NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.


Delrin® RA100CPE is a high viscosity acetal homopolymer for use in easy-to-fill moulds with very low VOC emissions, reduced lifecycle greenhouse gas emissions and lower fossil resource use. Delrin® RA100CPE provides optimum mechanical performance with its excellent combination of toughness and strength with improved processing, thermal stability and productivity for injection molding.

Delrin® Renewable Attributed base polymer is produced from 100% bio-feedstock from waste*. 100% certified renewable electricity is used for its production.
This approach helps customers in achieving their sustainability goals.

* according to ISCC Plus mass balance certification.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 1.9 cm³/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Molding shrinkage, parallel 2.2 % ISO 294-4, 2577
Molding shrinkage, normal 1.9 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2900 MPa ISO 527
Yield stress 71 MPa ISO 527
Yield strain 28 % ISO 527
Nominal strain at break 45 % ISO 527
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 450 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 16 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 13 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 178 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 95 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 160 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 110 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 100 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4.1 - IEC 62631-2-1
Relative permittivity, 1MHz 4 - IEC 62631-2-1
Dissipation factor, 100Hz 25 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 45 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity 6E14 Ohm IEC 62631-3-2
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 1 % Sim. to ISO 62
Humidity absorption 0.1 % Sim. to ISO 62
Density 1420 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Delrin® RA100CPE NC010, POM, DuPont
Shearstress-shear rate , Delrin® RA100CPE NC010, POM, DuPont
Stress-strain , Delrin® RA100CPE NC010, POM, DuPont
Secant modulus-strain , Delrin® RA100CPE NC010, POM, DuPont
Tensile modulus-temperature , Delrin® RA100CPE NC010, POM, DuPont
Characteristics
Processing
Injection Molding, Profile Extrusion, Sheet Extrusion, Other Extrusion
Delivery form
Pellets, Natural Color
Features
Low Emission, Thermal Stability, Homopolymer
Certifications
Contains renewable resources, ISCC Plus
Regional Availability
Other text information
Injection molding
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.
 

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com