Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Amphora™ 3D Polymer AM3300 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Amphora™ 3D Polymer AM3300:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Amphora datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Application/Uses
-Production of 3D Printing Filaments

Eastman Amphora™ AM3300 3D polymer is a low-odor, styrene-free material uniquely suited

for 3D printing enthusiasts, particularly those who need the flexibility to print within a wide

processing temperature range. Amphora AM3300 has good flow properties through the printer

nozzle—even at lower temperatures than some other polymers require. These properties

make AM3300 more workable at a wider breadth of temperatures, producing reliable results

and resulting in less waste.The model of functional aesthetics, Amphora AM3300 can be made

into high-quality filament that exhibits advanced overhang ability, excellent looks, and large

printing temperature range—empowering large panel of users to create durable and useful

items. Amphora AM3300 is also a highly efficient polymer that can help speed up processing

times. With the unique combination of a low processing temperature and an elevated

temperature resistance, Amphora AM3300, can quickly print creations that are functional,

durable, efficient, and attractive.

Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 50 MPa ASTM D 638
Tensile Strength at Break 35 MPa ASTM D 638
Elongation at Yield 4.5 % ASTM D 638
Elongation at Break 193 % ASTM D 638
Flexural Modulus 1800 MPa ASTM D 790
Flexural Strength 67 MPa ASTM D 790
Rockwell Hardness R 105 - ASTM D 785
Izod Impact notched, 1/8 in 70 J/m ASTM D 256
Izod Impact notched, Low-Temperature 38 J/m ASTM D 256
Temperature -40 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 71 °C ASTM D 648
DTUL @ 264 psi 63 °C ASTM D 648
Other propertiesValueUnitTest Standard
Density 1200 kg/m³ ASTM D 792
Characteristics
Processing
Additive Manufacturing
Special Characteristics
Heat stabilized or stable to heat
Features
High Gloss, Low Odor, Copolymer
Certifications
Food contact, Food approval FDA 21 CFR
Applications
Electrical and Electronical, Filament for 3D Printing
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.