Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of AKROLEN® PP GFM 25/15 LA black (3143) - PP-(GF+MX)40 - Akro-Plastic GmbH

Material Data Center offers the following functions for AKROLEN® PP GFM 25/15 LA black (3143):
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Akrolen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 13.5 cm³/10min ISO 1133
Temperature 230 °C -
Load 2.16 kg -
Molding shrinkage, parallel 0.2 % ISO 294-4, 2577
Molding shrinkage, normal 0.5 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 6500 MPa ISO 527
Stress at break 75 MPa ISO 527
Strain at break 75 % ISO 527
Flexural modulus, 23°C 6600 MPa ISO 178
Flexural strength 105 MPa ISO 178
Charpy impact strength, +23°C 45 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 45 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 10 kJ/m² ISO 179/1eA
Izod impact strength, +23°C 10 kJ/m² ISO 180/1U
Ball indentation hardness 100 MPa ISO 2039-1
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 167 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 150 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 163 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 20 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 125 E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Electric strength 18 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1210 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , AKROLEN® PP GFM 25/15 LA black (3143), PP-(GF+MX)40, Akro-Plastic
Shearstress-shear rate , AKROLEN® PP GFM 25/15 LA black (3143), PP-(GF+MX)40, Akro-Plastic
Specific volume-temperature (pvT) , AKROLEN® PP GFM 25/15 LA black (3143), PP-(GF+MX)40, Akro-Plastic
Characteristics
Delivery form
Black
Features
Laser Markable
Applications
Automotive, Electrical and Electronical
Regional Availability
Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.