Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PA11 ESD - PA11 - BASF

Material Data Center offers the following functions for Ultrasint PA11 ESD:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 20 / * cm³/10min ISO 1133
Temperatura 220 / * °C -
Carga 2.16 / * kg -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 204 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 111 / * °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 186 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat , A 192 / * °C ISO 306
Temperatura de amolecimento Vicat, B 183 / * °C ISO 306
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1070 / - kg/m³ ISO 1183
Bulk density 460 kg/m³ -
3D DataSeco / CondUnidadeMétodo de ensaio
Other Standards[S]
Módulo de tração, flat 3150 / 2300 MPa ISO 527
Módulo de tração, upright 2150 / 1550 MPa ISO 527
Resistência à tração, flat 65 / 55 MPa ISO 527
Resistência à tração, upright 55 / 47 MPa ISO 527
Deformação na ruptura, flat 20 / 22 % ISO 527
Deformação na ruptura, upright 23 / 31 % ISO 527
Módulo de flexão, flat 3050 / 2550 MPa ISO 178
Módulo de flexão, upright 2100 / 1650 MPa ISO 178
Resistência ao impacto Charpy, +23°C, flat 80 / 101 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, +23°C, upright 90 / 107 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C, flat 6.6 / 7.3 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, +23°C, upright 4.7 / 5.3 kJ/m² ISO 179/1eA
Resistência ao Impacto Izod, +23°C, flat 67 / 81 kJ/m² ISO 180/1U
Resistência ao Impacto Izod, +23°C, upright 58 / 83 kJ/m² ISO 180/1U
Impacto Izod com entalhe, +23°C, flat 7 / 7.9 kJ/m² ISO 180/1A
Impacto Izod com entalhe, +23°C, upright 5 / 5.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Características
Processamento
Additive Manufacturing, Sinterização a laser
Forma de entrega
Resistência Química
Resistência química geral
Certifications
Contém recursos renováveis
Aplicaciones
Elétrica e Eletrônica
Disponibilidade regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.