Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Ronfalin" in Material Data Center leads to the following information:

Tradename: Ronfalin
Family: ABS, ABS+PMMA, ASA, SAN
Producer: LyondellBasell Industries
65 hits in the material database
4 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
RONFALIN® ABS 1261 ABS
RONFALIN® ABS 1314 GB 10 ABS-GB10
RONFALIN® ABS 1326 ABS
RONFALIN® ABS 1328 ABS
RONFALIN® ABS 1328 A ABS
RONFALIN® ABS 1334 ABS
RONFALIN® ABS 1335 ABS
RONFALIN® ABS 1335 A ABS
RONFALIN® ABS 1335 A LM ABS
RONFALIN® ABS 1336 ABS
RONFALIN® ABS 1336 A ABS
RONFALIN® ABS 1336 CA ABS
RONFALIN® ABS 1336 FC ABS
RONFALIN® ABS 1337 ABS
RONFALIN® ABS 1344 FC ABS
RONFALIN® ABS 1352 A ABS
RONFALIN® ABS 1353 A ABS
RONFALIN® ABS 1361 ABS
RONFALIN® ABS 1362 CA ABS
RONFALIN® ABS 1363 ABS
RONFALIN® ABS 1363 A ABS
RONFALIN® ABS 1363 A U ABS
RONFALIN® ABS 1411 GF 30 ABS-GF30
RONFALIN® ABS 1412 GF 17 ABS-GF17
RONFALIN® ABS 1412 GF 20 ABS-GF20
RONFALIN® ABS 1413 GB 20 ABS-(GB+GB)20
RONFALIN® ABS 1424 FC ABS
RONFALIN® ABS 1443 U ABS
RONFALIN® ABS 1541 ABS
RONFALIN® ASA 3323 U ASA
RONFALIN® ASA 3324 U ASA
RONFALIN® ASA 3332 U ASA
RONFALIN® ASA 3421 U ASA
RONFALIN® ASA30U ASA
RONFALIN® ASA35U ASA
RONFALIN® ASA35UEF ASA
RONFALIN® C C110FR (PC+ABS) FR
RONFALIN® C C110FR GF20 (PC+ABS)-GF20 FR
RONFALIN® C C120 (PC+ABS)
RONFALIN® C C130 (PC+ABS)
RONFALIN® C C130 AM (PC+ABS)
RONFALIN® C C130 GF10 (PC+ABS)-GF10
RONFALIN® C C130 GF20 (PC+ABS)-GF20
RONFALIN® C C130 U (PC+ABS)
RONFALIN® C C135 (PC+ABS)
RONFALIN® C110 (PC+ABS)
RONFALIN® CP55 ABS
RONFALIN® FF50 ABS
RONFALIN® FF50AM ABS
RONFALIN® FFA59 ABS
RONFALIN® FFU50 ABS
RONFALIN® FG50 ABS
RONFALIN® FX50 ABS
RONFALIN® GGT07 ABS
RONFALIN® GS20 ABS
RONFALIN® HF20 ABS
RONFALIN® HX03 ABS
RONFALIN® HX10 ABS
RONFALIN® MABS 2224 MABS
RONFALIN® SAN 4501 GF35 SAN-GF35
RONFALIN® STA32 ABS
RONFALIN® TRE35 ABS
RONFALIN® TXE35 ABS
RONFALIN® TXE95 ABS
RONFALIN® TXG03 ABS-GF10

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.