Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Platilon" in Material Data Center leads to the following information:

Tradename: Platilon
Family: PUR
Producer: Covestro Deutschland AG
2 hits in the literature database
1 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2010-09-24, A Material Unlimited
...me system, PU metal composite elements and PU sealing systems. In addition, solvent-free adhesives are used for them. A highlight are the flexible thinlayer 2nd generation solar cells produced from Macrofol polycarbonate film and Platilon thermoplastic polyurethane (TPU). In a second step, flexible photovoltaic modules are created from these cells. The Solon Black 160/05 in-roof module with an “intelligent” system frame based on Bayflex PU foam has already been introduced to the market (Fig. 5)....

Kunststoffe international, 2011-05-12, Surfaces that Help Healing
...s they quickly absorb aqueous fluids which are often present in wound areas. At the same time they swell far less than conventional wound dressings. They are also gentle on the skin, resistant and at the same time flexible. They can be combined with Platilon films made from thermoplastic polyurethane that keep dirt and microbes away from the wound, but nevertheless allow the wound to breathe and are permeable to water vapor. The foams can be produced as roll material, but they can be shaped into...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.