Material datasheets available free. Online registration at: www.materialdatacenter.com
Geloy - ASA, ASA+PC - Saudi Basic Industries Corp. (Sabic)
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Geloy" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...ries of newly-developed ABS materials (grade: Cycolac) meet the requirements of the electrical industry for improved flame protection with lower emissions and a higher chemical resistance. GEP is additionally offering two new (PC+ASA) blends (grade: Geloy) with improved heat resistance and impact strength. The new developments in the field of PBT (grade: Valox) include a new extrudable product type which fulfils the requirements for hollow cables for optical waveguides. A further PBT type can be...
Kunststoffe international, 2005-11-21, Styrene Copolymers (ABS, ASA, SAN)
...siness from DSM, the brand name Ronfalin will continue. In ABS blends, seven different products from four manufacturers are significant on the market (Table 2). Blends with PC include Terblend S (BASF), Bayblend (Bayer), Pulse (Dow) and Cycoloy and Geloy (GE Plastics). (PA+ABS) blends are marketed by BASF as Terblend N and by Bayer as Triax. Market Segments Thanks to their versatile applications and processing properties, styrene copolymers have been able to compete very effectively with other...
Kunststoffe international, 2011-10-17, Styrene Copolymers (ABS, ASA, SAN, MABS, and ABS Blends)
...er (GF) reinforced grades have excellent flow properties even without large amounts of additives. The applications are, e.g., mirror covers and rear-view mirror fairings. Sabic recently expanded its (ASA+PC) portfolio (Geloy) with new grades for use in medicine, entertainment electronics and electrical applications. For light but matt surfaces in automotive interiors, dust-repellent antistatic grades are available. Blends of ABS and polyamides are characterized by an independent property profile...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.