Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Admer" in Material Data Center leads to the following information:

Tradename: Admer
Family: PO
Producer: Mitsui Chemicals Europe GmbH
53 hits in the material database
2 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2012-11-26, Joining of Dissimilar Materials
... (PP; grade: HD120MO, manufacturer: Borealis Polyolefine GmbH, Linz, Austria) and polyamide 6 (PA6; grade: Ultramid B3K, manufacturer: BASF SE, Ludwigshafen, Germany) were chosen. The adhesion promoter used for the intermediate films was of the type Admer QF551E (manufacturer: Mitsui Chemicals GmbH, Düsseldorf, Germany), which is PP-based and has grafted maleic anhydride groups. The test specimen geometry shown in Figure 4 was used for the welding tests. For the investigations of the weldability...

Kunststoffe international, 2014-04-14, Dynamic Differential Calorimetry: Using Flash DSC Technology to Verify Structural Changes
...nd a wall thickness of 1 mm, and are used as venting tubes in engine coolant circuits. They have a three-layer structure with an outer layer of PA612 (grade: Vestamid DX 9304, manufacturer: Evonik Industries AG, Essen, Germany), a primer (grade: Admer QB, manufacturer: Mitsui Chemicals Europe GmbH, Düsseldorf, Germany) as the central layer, and an inner layer of modified PP (grade: PP SX 8100, manufacturer: RTP France). In this laminated structure, the 0.45 mm thick outer layer provides mechanic...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.