Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Vamplen" in Material Data Center leads to the following information:

Tradename: Vamplen
Family: PP
Producer: Vamp Tech Spa
16 hits in the material database
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, A Home Game for the Italian Plastics Industry: Rendezvous in Milan
...Testing Technology Material and Proofing A flame-resistant low-density PP homopolymer whose dimensional stability almost matches that of PP with mineral fillers has been developed by Vamptech, Busnago. The material with the trade name Vamplen 0024 V2 LBC fulfils the provisions of UL 94 V2, is halogen-free and can be used at a sustained temperature of 110°C. Application areas are primarily small electrical devices (Fig.16) which are used in the household and are subject to directive IEC 60695-2...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.