Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Carp" in Material Data Center leads to the following information:

Tradename: Carp
Family: PF
Producer: Tufnol Ltd
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Requirements and Markets: Polymeric Flame Retardants
...cts are polymers with a high molecular weight, their molecules are too large to penetrate the cell membranes of living tissue. A study with 14C-tribromostyrene confirms that this compound does not accumulate in the tissues of experimental animals (carp). The regulatory agencies also recognise that bioaccumulation is unlikely, since they do not specify any bioaccumulation tests for polymers. The US Environmental Protection Agency (EPA) states that: "Polymers are not readily absorbed by biolog...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.