Material datasheets available free. Online registration at: www.materialdatacenter.com
Akulon - PA6, PA66 - DSM Engineering Materials
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Akulon" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...required electrical performance, and is the first and only company worldwide that has globally launched compounds for high-voltage applications with a certified CTI rating of >700 V (for Akulon PA 66) and >850 V (for ForTii PPA). These compounds are free of metals, halogens, red phosphorous and halide-based heat stabilizers, so that potential electrical corrosion of any metal used in the assembly of the components can be avoided. They are also available in orange colored grades. To ensure highes...
Kunststoffe international, 2005-11-21, Engineering Plastics: Products for Innovative Processes
...ed by around 22%, while mechanical properties differ only slightly from those of standard Durethan. In processing, the lower melting point of these grades enables cooling and cycle time to be reduced. DSM is supplying a new grade for laser welding: Akulon UltraLas K224-HWXG6, a 30% black-coloured, glass-fibre-reinforced grade. Because of the high laser-energy transmission of the PA6 base polymer (70% of a 1064nm-Nd-YAG laser), shorter cycle times, more complex geometries and lower section thickn...
Kunststoffe international, 2005-11-21, Interview: Newly Reorganised for the Future
...st promising engineering plastics markets for DSM are in Automotive, E&E and Packaging. The plastics-for-metal drive in automotive is ongoing, especially in the under-the-hood environment where we have very strong opportunities with our Stanyl PA46, Akulon PA6 and Arnitel TPEE. In addition, the increase in E&E markets, driven by consumer spending and the strong increase in electronics in daily life, stimulates the use of plastics where we can benefit again with Stanyl PA46, Arnite PBT and Xantar...
Kunststoffe international, 2005-11-21, Isocyanate-free Route to Polyurethane
...oxic CBC is suitable for use in reactive processing of polymer melts. At DSM, CBC was employed successfully as a chain extender for polyesters and polyamides and polyesters. As Fig.6 shows, CBC addition during melt processing of polyamide6 (grade: Akulon, manufacturer: DSM) produced a significant increase in solution viscosity; this is typical of the effective molecular weight build-up due to chain extension. Processing was carried out in a DSM twin-screw mini extruder at 270°C with a reside...
Kunststoffe international, 2005-11-21, Motor Vehicle Interiors
...nents remain unchanged. The excellent properties of TerblendN, faithfully reproduce fine surface structures and thus, even when unpainted parts are used, the product gives the impression of a mat surface (Fig.5). Akulon (PA6GF), Arnitel (thermoplastic elastomer; TPE) and StapronE, a PC/ PET alloy, are DSM’s materials for interior safety parts. Airbag containers of AkulonK224-PG8 play an important role in passenger safety. The parts fulfil not only the high strength requirements but have extremel...
Kunststoffe international, 2005-11-21, Under the Microscope
...arrier materials (e. g. EVOH), the oxygen permeability of polyamide 6 depends substantially on the relative atmospheric humidity and this fact severely limits its usefulness as a monolayer material. Figure 1 shows the oxygen permeability of the PA 6 Akulon F136-C as a function of relative atmospheric humidity. It may be seen that oxygen permeability decreases at low relative humidity but increases strongly at high levels. For a long time, there was no explanation for this behaviour of polyamide ...
Kunststoffe international, 2007-09-19, Energy Efficiency Taking on Increasing Importance
...rmed with the standard crash simulation programs available on the market. A series of new and particularly easy-flow materials has been brought onto the market by DSM Engineering Plastics BV, Sittard/Netherlands. The new materials include Akulon XP – a PA6 – (with high viscosity) for packaging applications, Akulon Ultraflow – a PA6 – and Stanyl High Flow and Super Flow – PA46 grades. Akulon Ultraflow PA6, for instance, with its excellent flowability (80 % higher than standard PA6), permits a 25...
Kunststoffe international, 2007-09-19, For High-End Applications
...ore highly in terms of stiffness. A new technology enables glass fibers to be incorporated into the polymer matrix. The structural strength so acquired nearly approaches that of metals but cuts weight by half. Price Breakers With Arnite XL PBT, Akulon Ultraflow PA6 and Stanyl PA46, DSM Engineering Plastics of Sittard, Netherlands, would like to offer lower-priced alternatives to high-temperature plastics such as PPA, PPS, PEI and PEEK. In the context of AFL/DBL (flame retardancy classification...
Kunststoffe international, 2010-08-19, Grow Strategically
...n solar collectors (Fig. 1). DSM: Asia in its Sights DSM Engineering Plastics of Sittard, the Netherlands, has used the time since the K2007 to become further established in Asia. For instance, a plant for manufacturing polyamide (PA) 6 (type: Akulon; use: packaging films) was put into operation in Jiangyin, China, in 2008. In 2009, a compounding plant was built in India, and in that year the company dedicated a new building of higher learning for research and development in Shanghai, China. T...
Kunststoffe international, 2010-09-24, Sustainable and Efficient
...to tests by a German OEM, then validated and admitted for applications with permanent operating temperatures of up to 230°C, which mainly refers to application in resonators, intercooler ducts and flaps. DSM will moreover bring to the market Akulon Diablo, which is a PA6 high-temperature material. This special version of Akulon was designed for use in air-fuel systems continuously submitted to temperatures up to 210°C, and even 230°C, at short term. Selected customers are currently receiving spe...
Kunststoffe international, 2014-10-10, Polyamides (PA)
...ced partly aromatic polyamide (66/6I), which is outstanding for its delayed crystallization behavior. This enables high-quality class-A surfaces, despite a high fiber content. DSM recently presented two UV-stabilized PA6 types (Akulon) designed for the production of exterior mirror casings and vehicle door handles, which do not have to be varnished after production. High-Temperature ApplicationsIn this area, polyamides are finding their way into applications that used to be dominated by heat-res...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.