Xenoy - PC+PBT, PC+PET - Saudi Basic Industries Corp. (Sabic)
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Xenoy" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
An unusual balance of high modulus and ductile impact behavior is claimed for Xenoy HMD resins, recently launched by SABIC Innovative Plastics. As we reported initially in November, these PC/PBT and P...
Kunststoffe international, 2005-11-21, Automated Injection Moulding and Welding of Bumpers
...k of automating the injection moulding process and downstream operations in as comprehensive and space-saving a way as possible. The 1850 mm wide, 300 mm high and 920 mm deep bumper, which weighs around 5 kg, is produced from a PC+PBT blend (grade: Xenoy, manufactured by General Electric Plastics) on a two-plate injection moulding machine with 40 000 kN clamping force (type: KM 4000/25000 MC, manufactured by Krauss-Maffei Kunststofftechnik GmbH, Munich) (Fig. 1). Then three separately produced p...
Kunststoffe international, 2005-11-21, No Need for Painting?
...e film is going to be available in a wide range of metallic and other colour effects, and will thereby support new trends in automotive design. Sollx film technology has been developed from the first generation of self-coloured PC/PBT blends (grade: Xenoy) from GE plastics, which themselves represented a significant advance for automotive designers. The substitution of thermoplastics for metals led to significant advantages. The use of PC/PBT blends not only achieves a weight reduction, but the ...
Kunststoffe international, 2005-11-21, The Crucial Question in Fire Protection
... Greater uniformity among the standards in this sector could help to focus on further development in this direction with a view to making them more affordable. The Author of this Article François de Bie is Product Manager for Valox/Xenoy Resins at GE Plastics Europe, Bergen op Zoom/Netherlands. Contact: francois.debie@gepex.ge.com Fig.1. Plug made from flame-resistant, glassfibre-reinforced (PS+PPO) blend Table 1. Typical properties of PBT-GF30 containing flame retardant as virgin ma...
Kunststoffe international, 2008-08-14, Consolidated Strategies
...echnology Manager for Crystalline Products, stressed that the company is involved in several research projects. Environmentally friendly innovations and progressive technologies are not mutually exclusive, as shown by Valox-iQ (PBT) and Xenoy-iQ (PC/PBT blend). Manufacturing these products, up to 85 % of raw materials based on chemically recycled PET is used. The new Sabic IP technology is able to turn PET particles, such as are obtained from recycled PET bottles, into monomers f...
Kunststoffe international, 2008-09-23, Plastics, Electronics and the Environment
...nce plastic using recycled material that fulfills the UL safety standards. Sabic Innovative Plastics and other businesses still search for possible technologies for this difficult environmental problem. Examples from recent examples are Valox iQ and Xenoy iQ, the polyester PC, PET and PBT based on recycled material and their blends by Sabic Innovative Plastics. These products use PBT, in which 85% of the chemicals used in a patented chemical process are recovered from recycled PET bottles and fi...
Kunststoffe international, 2019-12-18, Electromobility and a Concept Vehicle
...th combustion engines. For this reason, automakers protect the battery packs with special underbody shields and other safety devices such as e. g. side skirts. At the K, Sabic from Riyadh, Saudi Arabia, presented the polyester-based material Xenoy HTX for such skirts. The material originates from the company’s Xenoy series, and is available as unreinforced and glass fiber-reinforced version. In order to demonstrate the material’s performance, the company showed the 3D-printed prototype of a side...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.