Material datasheets available free. Online registration at: www.materialdatacenter.com
Silastic - SI - Dow Corning Corporation
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Silastic" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...h might be reasons for property changes. By a suitable selection of the process parameters these micro cracks can be minimized or even avoided. To evaluate the process the treatment of the 3 mm thick LSR disk (grade: Silastic MS-1002; manufacturer: Dow Chemical) both the radiation time as well as the surface is varied. Plotting the spectral transmission (Fig. 2) demonstrates, that below 450 nm the transmission is not affected at all, while below 450 nm the transmission is slightly reduced, which...
Kunststoffe international, 2005-11-21, Driving the Automotive Industry: Engineering Elastomers
Trend Report Crosslinking Plastics Engineering Elastomers Driving the Automotive Industry. Within the elastomer-manufacturing industry, there is increasing concentration and focus on product groups. Regardless of this, the trend towards relocating production of standard products within the expanded European Union continues to advance. In the future, China and India will also increasingly emerge both as markets and production locations for engineering elastomer products. Werner P. Lauhus The Eu...
Kunststoffe international, 2005-11-21, Elastomers
...(Q, LSR, HTV): DowCorning, Midland, MI/USA, as a producer, offers more than 5000 silicone rubber compound formulations based on its Silastic product range. They include liquid silicone rubber (LSR) and solid silicone rubbers, as well as fluorinated silicone rubbers. The new Silastic4-4768 is translucent and is a 70ShoreA grade (tear strength 9.5MPa at 350% elongation) for extrusion, injection moulding and calendaring. SilasticHGS700 (beige) is also a 70Shore A grade with a good range of properti...
Kunststoffe international, 2006-04-04, Market Launch: Foamed Liquid Silicone Opens New Doors
...ed in the material. The overall system, which consists of the two loading units and the mixing block, can be retrofitted easily to injection moulding machines that are equipped for processing LSR (Fig.5). Dow Corning provided a trial product (grade: Silastic LC 2004 FX ) with optimum crosslinking kinetics that was geared to the demands of the foaming process. Its homoge-neous foam structures reduce the density of the material by between 10 and 50% (Fig. 6). The Shore hardness can be reduced by u...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.