Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Reny" in Material Data Center leads to the following information:

Tradename: Reny
Family: PA
Producer: Mitsubishi Engineering-Plastics Corporation
25 hits in the material database
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Reny 1002H PAMXD6-GF30
Reny 1012H PAMXD6-GF40
Reny 1021UCS PAMXD6-GF50
Reny 1022H PAMXD6-GF50
Reny 1025 PAMXD6-GF50
Reny 1027 PAMXD6-GF50
Reny 1032 PAMXD6-GF60
Reny 1071 PAMXD6-GF55
Reny 1313 PAMXD6-GF40
Reny 1501AH PAMXD6-GF30
Reny 1511AH PAMXD6-GF40
Reny 1521AH PAMXD6-GF50
Reny 1722F PAMXD6-GF50
Reny 2502A PAMXD6-(GF+MF)20
Reny 2620 PAMXD6-(GF+MF)20
Reny 4011 PAMXD6-GF40
Reny 4511 PAMXD6-GF40
Reny C36 PAMXD6-CF30
Reny E40 PAMXD6-MF40
Reny G07S PAMXD6-GF20
Reny G16S PAMXD6-CF20
Reny N252 PAMXD6-(GF+MF)25
Reny NXG5050 PAMXD6-GF50
Reny W110 PAMXD6-Z
Reny W38S2 PAMXD6-Z30

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.