Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PAHT CF15 - PA*-CF15 - BASF

Material Data Center offers the following functions for Ultrafuse PAHT CF15:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 42.2 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 234 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 70 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 92 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 145 / * °C ISO 75-1/-2
Other propertiesdry / condUnitTest Standard
Density 1230 / 1230 kg/m³ ISO 1183
3D Datadry / condUnitTest Standard
Other Standards[S]
Tensile modulus, flat 8390 / 5050 MPa ISO 527
Tensile modulus, upright 3530 / 2460 MPa ISO 527
Tensile strength, flat 103 / 62.9 MPa ISO 527
Tensile strength, upright 18.2 / 19.1 MPa ISO 527
Strain at break, flat 1.8 / 2.9 % ISO 527
Strain at break, upright 0.5 / 0.8 % ISO 527
Flexural modulus, flat 8260 / 6060 MPa ISO 178
Flexural modulus, on-edge 7670 / 6260 MPa ISO 178
Flexural modulus, upright 2710 / 2190 MPa ISO 178
Flexural strength, flat 161 / 125 MPa ISO 178
Flexural strength, on-edge 172 / 122 MPa ISO 178
Flexural strength, upright 50.8 / 56 MPa ISO 178
Charpy impact strength, +23°C, flat 20.6 / 21.9 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, on-edge 19.3 / 20.4 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, upright 2.9 / 2.8 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C, flat 4.8 / 5.1 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, on-edge 3.9 / 5.3 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, upright 1.3 / 1.6 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, flat 16.4 / 16.3 kJ/m² ISO 180/1U
Izod impact strength, +23°C, on-edge 18.1 / 15.1 kJ/m² ISO 180/1U
Izod impact strength, +23°C, upright 2.9 / 4.1 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, flat 4.9 / 6.5 kJ/m² ISO 180/1A
Izod notched impact strength, +23°C, on-edge 5.1 / 5.8 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Additive Manufacturing
Delivery form
Monofilament
Special Characteristics
Heat stabilized or stable to heat
Chemical Resistance
General Chemical Resistance
Regional Availability
North America, Europe, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.