Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ MP100 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ MP100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastman Tritan™ MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation copolyester can be thermoformed with a wide processing window that allows for product designs that reflect intricate detail.

Eastman Tritan™ MP100 copolyester is suitable for use with most forms of sterilization including radiation and ethylene oxide. It is NOT suitable for autoclave/steam sterilization. Eastman Tritan™ MP100 copolyester has been

formulated for use in medical film, sheet, and packaging applications.

Thermal propertiesValueUnitTest Standard
ASTM Data
Coefficient of Thermal Expansion, MD 88 E-6/K ASTM D 696
Glass Transition Temperature 110 °C ASTM E 1356
Optical propertiesValueUnitTest Standard
ASTM Data
Gloss 161 - ASTM D 2457
Haze 1 % ASTM D 1003
Light Transmittance 92 % ASTM D 1003
Index of Refraction 1.54 - ASTM D 542
Other propertiesValueUnitTest Standard
Water Absorption, 24hr 0.5 % ASTM D 570
Density 1190 kg/m³ ASTM D 792
Film PropertiesValueUnitTest Standard
ISO Data
Trouser Tear resistance, parallel 11 N/mm ISO 6383-1
Trouser Tear resistance, normal 11 N/mm ISO 6383-1
Thickness of specimen 0.25 mm -
ASTM Data
Tensile Modulus, MD 1460 MPa ASTM D 882
Tensile Modulus, TD 1380 MPa ASTM D 882
Tensile Strength at Yield, MD 41 MPa ASTM D 882
Tensile Strength at Yield, TD 40 MPa ASTM D 882
Tensile Strength at Break, MD 59 MPa ASTM D 882
Tensile Strength at Break, TD 52 MPa ASTM D 882
Elongation at Yield, MD 7 % ASTM D 882
Elongation at Yield, TD 7 % ASTM D 882
Elongation at Break, MD 179 % ASTM D 882
Elongation at Break, TD 203 % ASTM D 882
Thickness of specimen 0.25 mm -
Characteristics
Processing
Film Extrusion, Sheet Extrusion, Thermoforming
Special Characteristics
Heat stabilized or stable to heat, Transparent, Sterilizable, Ethylene Oxide (EtO) Sterilization, Gamma irradiation sterilization
Features
Amorphous, Heat Sealable, Copolymer
Chemical Resistance
General Chemical Resistance, Radiation Resistance
Applications
Medical, Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.