Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Recyclostab - Process and heat stabilizers - Ciba

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Recyclostab" in Material Data Center leads to the following information:

Tradename: Recyclostab
Family: Process and heat stabilizers
Producer: Ciba
2 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Integrated Solutions
...share of recyclable material in end-of-life cars. By 2015, some 95% of the plastics are to be recycled and fed back into automotive applications. As a result, increased use is already being made of polyolefins today. Additives such as Recyclostab or Recycloblend provide support in the recycling of bumpers, battery cases and petrol tanks, making it possible to achieve virtually the same properties as in virgin material. Figure 5 compares the properties of painted bumpers in new material with thos...

Kunststoffe international, 2015-12-17, Improving the Quality of Recycled Materials
...ion with co-stabilizers, e. g. acid scavengers. Light stability is enhanced with hindered amines (HA(L)S), e. g. low- or high-molecular weight, sterically hindered piperidines, and/or UV absorbers, e. g. based on benzophenone or benzotriazole. The Recyclostab and Recyclossorb series of products from PolyAd Services GmbH, Lampertheim, Germany, have a proven track record as stabilizers for recycled materials. Thus, Recyclostab 411 improves the processing stability of recycled HDPE material and pol...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.