Material datasheets available free. Online registration at: www.materialdatacenter.com
Licomont - Antislip agents, antiblock agents, lubricants - Clariant International Ltd
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Licomont" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...hanical properties (Fig. 2). As waxes, these additives also have further positive influences. They help to homogeneously distribute other additives and fillers, improve on the flow properties and reduce the demoulding force (Fig. 3). The montan wax, Licomont CaV 102 (manufacturer: Clariant, Gersthofen) thus not only acts as a nucleation agent here but also serves as a demoulding aid. By contrast to the stearates that are otherwise used, the montan acid salts are scarcely prone to migration and a...
Kunststoffe international, 2005-11-21, Injection Moulding Metal and Ceramic Powder
...process, it is coated with a thermoplastic binder before further processing. This is normally based on polyolefins or polyoxymethylene. A very wide variety of binder systems are commercially available. Particular advantages are offered by the binder Licomont EK 583 (manufactured by Clariant). This system is based on a polymer wax and contains both water-soluble and insoluble components. It can be processed with any sinterable powder and is exceptionally easy to process. Mixing and subsequent bin...
Kunststoffe international, 2005-11-21, Market and Trends: Nanomaterials: Opportunities and Risks
...s based on isotactic polypropylene (grade: PP HC001, manufacturer: Borealis), the compatibiliser PP-g-MA (grade: Licomont AR 504, manufacturer: Clariant), the thermoplastic elastomer SEBS (grade: Kraton G-1652, manufacturer: Shell) and fluorohectorite (grade: Somasif, manufacturer: Co-op Chemicals), modified by means of cation exchange with protonated octadecylamine Colloidal crystals Fig.19. Photonic crystals consist of colloid crystals with periods in the wavelength range and are employed as...
Kunststoffe international, 2005-11-21, Wood Plastic Composites on the Right Track?
...ollowing materials were used in the trials: a metallocene polyproplyene (PP; grade: MR 2002, manufacturer: Total Petrochemicals, MFR=13g/10min), wood pellets (type: Lignocel P Super, manufacturer: Rettenmaier) and coupling agent (PP-MAH; type: Licomont AR 504, manufacturer: Clariant). The wood pellets were predried in a circulating-air dryer (type: LS 50, manufacturer: Motan) to give a residual moisture content in all the trials of less than 1%. The compounds were produced in a planetary roller...
Kunststoffe international, 2006-11-24, Additive Systems: Composition Decides
...lity requirements, it is of particular significance that component stiffness is homogeneous and reproducible. This is exactly what is achieved when combining wood to a plastics material that is precisely adjusted. Additive agents, e.g. Licomont AR 504 by Clariant, have proved to help step up stiffnesses in WPC, if compared to additive-free formulations, by improving the bond between wood fibre and plastics matrix. Block or graft copolymers made out of different polymers grafted with e.g. malei...
Kunststoffe international, 2007-04-17, Ceramics Dressed as Plastics
...O2) and silicon nitride (Si3N4) inserts were produced for the overmoulding trials. To develop the feedstock, an appropriate binder system first had to be chosen. For simple ceramic bar geometries, a commercial system proved suitable (grade: Licomont; manufacturer: Clariant AG). Production of the sleeves required a binder ensuring that the green compact had a higher strength. In this case, therefore, a binder separately developed by the Forschungszentrum Karlsruhe was used: a mixture of polyolefi...
Kunststoffe international, 2014-03-21, MagnetPIM: One-Shot Production of Sintered Magnets
...en powder for the production of plasticbonded permanent magnets and is also marketed for this purpose. The manufacturer did not optimize the material for the sintering process. Debindering with the Least-Possible Residual Carbon The binder (grade: Licomont EK583G; manufacturer: eMBe Products & Service GmbH) needs to be extracted in two stages: first in a water bath, then thermally. This approach in which the binder component is extracted with a solvent first stems from the insight that thermal d...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.