Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ EXL Filament AMHI240F Black - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ EXL Filament AMHI240F Black:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
LEXAN™ EXL AMHI240F filament is a high impact polycarbonate product available in black and white colors. It provides high impact strength and improved ductility over standard polycarbonate at room temperature and extreme low temperatures.
Other propertiesValueUnitTest Standard
Density 1190 kg/m³ ASTM D 792
3D DataValueUnitTest Standard
Other Standards[S]
Tensile modulus, flat 1730 MPa ASTM D 638
Tensile modulus, on-edge 1910 MPa ASTM D 638
Tensile modulus, upright 1800 MPa ASTM D 638
Stress at break, flat 45 MPa ASTM D 638
Stress at break, on-edge 55 MPa ASTM D 638
Stress at break, upright 40 MPa ASTM D 638
Strain at break, flat 7 % ASTM D 638
Strain at break, on-edge 5 % ASTM D 638
Strain at break, upright 3 % ASTM D 638
Flexural modulus, flat 1530 MPa ASTM D 790
Flexural modulus, on-edge 1910 MPa ASTM D 790
Flexural modulus, upright 1500 MPa ASTM D 790
Charpy impact strength, +23°C, flat 88 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, on-edge 151 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, upright 23 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C, flat 19 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, on-edge 30 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, upright 6 kJ/m² ISO 179/1eA
Temp. of deflection under load, 1.80 MPa, flat 139 °C ASTM D 6484
Temp. of deflection under load, 1.80 MPa, on-edge 138 °C ASTM D 6484
Temp. of deflection under load, 1.80 MPa, upright 138 °C ASTM D 6484
Vicat softening temperature, A, flat 148 °C ASTM D 1525
Vicat softening temperature, A, on-edge 149 °C ASTM D 1525
Vicat softening temperature, A, upright 149 °C ASTM D 1525
Coeff. of linear therm. expansion, parallel, flat 77 E-6/K ASTM E 831
Coeff. of linear therm. expansion, parallel, on-edge 80 E-6/K ASTM E 831
Coeff. of linear therm. expansion, parallel, upright 79 E-6/K ASTM E 831
Coeff. of linear therm. expansion, normal, flat 77 E-6/K ASTM E 831
Coeff. of linear therm. expansion, normal, on-edge 81 E-6/K ASTM E 831
Coeff. of linear therm. expansion, normal, upright 79 E-6/K ASTM E 831
Burning Behav. at thickness h, flat V-0 class UL 94
Burning Behav. at thickness h, on-edge V-0 class UL 94
Burning Behav. at thickness h, upright V-2 class UL 94
Thickness tested 3.0 mm UL 94
Volume resistivity, flat 1.4E13 Ohm*m ASTM D 257
Volume resistivity, on-edge 1.5E13 Ohm*m ASTM D 257
Volume resistivity, upright 1.5E13 Ohm*m ASTM D 257
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Additive Manufacturing
Delivery form
Monofilament, Black
Special Characteristics
High impact or impact modified
Features
Ductile
Regional Availability
North America, Europe, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.