Material datasheets available free. Online registration at: www.materialdatacenter.com
Kepital - POM - Korea Engineering Plastics Co. Ltd
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Kepital" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...on was paid to temperature control. Two other important criteria were ease of maintenance and the possibility of rapidly exchanging wear components. This short list summarises all the product data: - article: screw-in tip for darts; - material: POM Kepital F30-03 Natural (manufacturer: Tekuma Kunststoff GmbH, Reinbek/Germany); - batch: Orange AEZ052 (manufacturer: Clariant Masterbatches (Deutschland) GmbH, Lahnstein/Germany; - product dimensions: length 28mm, diameter 3.5 to 4.5 to 2.5 to 0.8mm;...
Kunststoffe international, 2014-10-10, Polyoxymethylene (Polyacetal, POM)
...th Korea.The current market leaders are Celanese Corp., Dallas, Texas/USA (Hostaform, Kematal, Celcon); DuPont AG, Wilmington, Delaware/USA (Delrin); Polyplastics AG, Tokyo, Japan (Duracon), Korea Engineering Plastics Co. Ltd., Seoul, South Korea (Kepital); Mitsubishi Chemicals Inc., Tokyo, Japan (Lupital); and BASF SE, Ludwigshafen, Germany (Ultraform). Other notable producers are Zaklady Azotowe w Tarnowie-Mościcach S.A., Tarnów, Poland (Tarnoform); Kolon Plastics Inc., Gimcheon, South Korea (...
Kunststoffe international, 2017-11-29, An Attritional Rendezvous
...tion material. This results from the low frictional resistance and the high abrasion, wear, and fatigue resistance of the polyacetal. The major trade names and their manufacturers are: Delrin (DuPont), Hostaform (Celanese), Ultraform (BASF), and Kepital (KEP). By adding PTFE, it is possible to combine its good sliding properties with the high mechanical strength of POM [1].PTFE belongs to the group of semicrystalline thermoplastics and is marketed under the trade names Algoflon (Solvay Solexis),...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.