Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® R433H BK0746 - PA66-GF33 - Ascend

Material Data Center offers the following functions for Vydyne® R433H BK0746:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Vydyne R433H BK0746 is designed to reinforce downgauged steel and aluminum used in vehicle body-in-white (BIW) structures, helping reduce weight without sacrificing safety or comfort.
R433H BK0746 has improved energy absorption over traditional glass-filled PA66, helping reduce noise, vibration and harshness (NVH) and absorbing impact energy from crashes. Using R433H BK0746 in the BIW structure reinforces sheet metal, helping manufacturers shave substantial weight and improve efficiency. Trends in lightweight and NVH are becoming even more paramount with the growth of Electric Vehicles. Vydyne R433H BK0746 has excellent performance attributes to support applications where this will be of prime importance such as battery frames and housings.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
模塑收缩率, 平行 0.6 / * % ISO 294-4, 2577
模塑收缩率, 垂直 1.0 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 9600 / 6200 MPa ISO 527
屈服应力 150 / 103 MPa ISO 527
屈服伸长率 3.3 / 7.4 % ISO 527
弯曲模量, 23°C 8400 / 6000 MPa ISO 178
弯曲强度 210 / 130 MPa ISO 178
无缺口简支梁冲击强度, +23°C 96 / 96 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 100 / 92 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 24 / 27 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 17 / 16 kJ/m² ISO 179/1eA
悬臂梁缺口冲击强度, +23°C 21 / 29 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 15 / - kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 - 温度 -40 °C -
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 262 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 245 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 260 / * °C ISO 75-1/-2
线性热膨胀系数, 平行 16 / * E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 11 / * E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.5 / * mm -
厚度为h时的燃烧性 V-2 / * class IEC 60695-11-10
测试用试样的厚度 0.4 / * mm -
ASTM数据
UL94 燃烧性 V-2 - UL 94
测试厚度 0.4 mm -
电性能干 / 已调节单位Test Standard
ISO数据
介电强度 28 / - kV/mm IEC 60243-1
其它性能干 / 已调节单位Test Standard
吸水性 1 / * % 类似ISO 62
吸湿性 1.3 / * % 类似ISO 62
密度 1350 / - kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 °C -
预干燥-时间 4 h -
注塑熔体温度 285 - 305 °C -
模具温度 65 - 95 °C -
1区 280 - 310 °C -
2区 280 - 310 °C -
3区 280 - 310 °C -
喷嘴温度 280 - 310 °C -
典型数据
加工方法
注塑
供货形式
粒料, 黑色
添加剂
润滑剂
特殊性能
高冲击韧性的/经抗冲改性的, 经热稳处理的/耐热的
特征
阻隔声音
耐化学试剂
通用耐化学性, 耐溶剂性, 耐油性
应用
汽车, 封装
地区供应
北美, 欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.