Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LLDPE 518N - (PE-LLD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LLDPE 518N:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
SABIC® LLDPE 518N is a butene linear low density polyethylene resin. Films produced from this resin have high toughness,good puncture resistance, good heat sealing behaviour and excellent machinability on conversion lines. Typical applications for SABIC® LLDPE518N are heavy duty shipping sacks, ice bags, frozen food bags, potato bags and agriculture films. Film properties: Film of 50 µm and BUR=2 has been produced on Kiefel IBC with 130 kg/h. Die size 200 mm, die gap 2,7 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.
热性能价值单位Test Standard
ISO数据
维卡软化温度, A 104 °C ISO 306
光学特性价值单位Test Standard
ASTM数据
雾度 13 % ASTM D 1003
机械性能(薄膜)价值单位Test Standard
ISO数据
拉伸模量, 平行 170 MPa ISO 527-3
拉伸模量, 垂直 180 MPa ISO 527-3
屈服应力, normal 11 MPa ISO 527-3
断裂应力, 平行 40 MPa ISO 527-3
断裂应力, 垂直 32 MPa ISO 527-3
继续撕裂强度, 平行 30 N/mm ISO 6383-1
继续撕裂强度, 垂直 180 N/mm ISO 6383-1
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.