Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Softlight 8N df21 - PMMA - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Softlight 8N df21:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Productprofil:

PLEXIGLAS® Softlight 8N df21 molding compound, based on PLEXIGLAS® 8N, is characterized by diffuse scattering of light.

 

Typical properties of PLEXIGLAS® molding compound are

 

  1. good flow
  2. high mechanical strength, surface hardness and mar resistance
  3. very good weather resistance.

 

Special properties of PLEXIGLAS® Softlight 8N df21 are

 

  1. good lightdiffusion combined with excellent light transmission.


Application:

Used for injection molding items for lighting engineering applications

Example:

displays, backlight units

Processing:

PLEXIGLAS® Softlight 8N df21 can be processed on injection molding machines with 3-zone general purpose screws for engineering thermoplastics.

Physical Form / Packaging:

PLEXIGLAS® Softlight df molding compounds are supplied as pellets of uniform size, packaged in 25kg polyethylene bags; other packaging on request.

加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 2.5 cm³/10min ISO 1133
温度 230 °C -
载荷 3.8 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 3300 MPa ISO 527
断裂应力 71 MPa ISO 527
断裂伸长率 4.5 % ISO 527
无缺口简支梁冲击强度, +23°C 18 kJ/m² ISO 179/1eU
热性能价值单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min 111 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 98 °C ISO 75-1/-2
热变形温度, 0.45 MPa 103 °C ISO 75-1/-2
维卡软化温度, B 109 °C ISO 306
线性热膨胀系数, 平行 63 E-6/K ISO 11359-1/-2
电性能价值单位Test Standard
ISO数据
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 1E13 Ohm IEC 62631-3-2
光学特性价值单位Test Standard
ISO Data
光输送 87 % ISO 13468-1, -2
其它性能价值单位Test Standard
密度 1190 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 248 °C ISO 294
注塑, 模具温度 69 °C ISO 294
注塑, 注射速度 195 mm/s ISO 294
函数
粘度-剪切速度 , PLEXIGLAS® Softlight 8N df21, PMMA, Röhm
剪切应力-剪切速度 , PLEXIGLAS® Softlight 8N df21, PMMA, Röhm
动态剪切模量-温度 , PLEXIGLAS® Softlight 8N df21, PMMA, Röhm
应力-应变.  , PLEXIGLAS® Softlight 8N df21, PMMA, Röhm
正割模量-应变.  , PLEXIGLAS® Softlight 8N df21, PMMA, Röhm
拉伸模量-温度 , PLEXIGLAS® Softlight 8N df21, PMMA, Röhm
典型数据
加工方法
注塑
供货形式
粒料
添加剂
脱模助剂
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的
特征
光散射
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
PREPROCESSING
Predrying temperature: max. 95 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 260°C
Mold temperature:60 - 90°C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.