Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® 8N - PMMA - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® 8N:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
产品概述: PLEXIGLAS® 8N 是一种无定形热塑性模塑料(PMMA). PLEXIGLAS® 模塑料常见的性能如下: •良好的流动性

•优异的机械性能

, 表面硬度和抗磨损性 •高透光率

•强耐候性

•晶莹透明的透明性赋予了该产品丰富的着色性

PLEXIGLAS® 8N 特殊性能如下: •良好的机械性能

•最高的热变形温度

•优良的流动性能

/熔融粘度 AMECA listing应用:

用于注塑成型的光学和科技产品

应用实例

:导光板, 照明灯罩, 汽车车灯, 工具箱外壳, 光学透 ,橱窗等 加工方法: PLEXIGLAS® 8N 可用常见的三段式注塑机注塑成型为 工程用的热塑性塑料

模塑料物理形态

/包装: PLEXIGLAS® 8N 模塑料成品是粒径均匀的粒料, 以聚 乙烯袋每25公斤包装或以配有聚乙烯内衬的箱子每500公斤包装;也可应顾客要求包装。
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 3 cm³/10min ISO 1133
温度 230 °C -
载荷 3.8 kg -
熔体密度 1060 kg/m³ -
熔体 0.181 W/(m K) -
熔体的比热 2440 J/(kg K) -
有效导热率a 6.99E-8 m²/s -
喷射温度 90 °C -
机械性能价值单位Test Standard
ISO数据
拉伸模量 3300 MPa ISO 527
断裂应力 77 MPa ISO 527
断裂伸长率 5.5 % ISO 527
拉伸蠕变模量, 1h 2800 MPa ISO 899-1
拉伸蠕变模量, 1000h 2200 MPa ISO 899-1
无缺口简支梁冲击强度, +23°C 20 kJ/m² ISO 179/1eU
热性能价值单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min 117 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 98 °C ISO 75-1/-2
热变形温度, 0.45 MPa 103 °C ISO 75-1/-2
维卡软化温度, B 108 °C ISO 306
线性热膨胀系数, 平行 80 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.6 mm -
Yellow Card 现存 是的 - -
燃烧性-氧指数 17.2 % ISO 4589-1/-2
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 3.6 - IEC 62631-2-1
相对介电常数., 1MHz 2.7 - IEC 62631-2-1
介质损耗因子, 100Hz 500 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 200 E-4 IEC 62631-2-1
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 1E13 Ohm IEC 62631-3-2
相对漏电起痕指数 600 - IEC 60112
光学特性价值单位Test Standard
ISO Data
光输送 92 % ISO 13468-1, -2
其它性能价值单位Test Standard
吸水性 2 % 类似ISO 62
吸湿性 0.6 % 类似ISO 62
密度 1190 kg/m³ ISO 1183
模塑测量的特殊性能价值单位Test Standard
ISO数据
粘数 53 cm³/g ISO 307, 1157, 1628
试样制备条件价值单位Test Standard
ISO数据
ISO试样制备条件. 8257 - ISO ....-2
注塑, 熔体温度 248 °C ISO 294
注塑, 模具温度 68 °C ISO 294
注塑, 注射速度 195 mm/s ISO 294
函数
粘度-剪切速度 , PLEXIGLAS® 8N, PMMA, Röhm
剪切应力-剪切速度 , PLEXIGLAS® 8N, PMMA, Röhm
动态剪切模量-温度 , PLEXIGLAS® 8N, PMMA, Röhm
应力-应变.  , PLEXIGLAS® 8N, PMMA, Röhm
正割模量-应变.  , PLEXIGLAS® 8N, PMMA, Röhm
应力-应变(等时的) 23°C, PLEXIGLAS® 8N, PMMA, Röhm
蠕变模量-时间. 23°C, PLEXIGLAS® 8N, PMMA, Röhm
蠕变曲线 23°C, PLEXIGLAS® 8N, PMMA, Röhm
比容-温度(pvT) , PLEXIGLAS® 8N, PMMA, Röhm
拉伸模量-温度 , PLEXIGLAS® 8N, PMMA, Röhm
典型数据
加工方法
注塑
供货形式
粒料
添加剂
脱模助剂
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的, 透明.
特征
无定形
应用
汽车
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
PREPROCESSING
预干燥温度: 最高98℃
在除湿型干燥器中的预干燥时间: 2-3h
PROCESSING
Melt temperature: 220 - 260°C
Mold temperature:60 - 90°C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.