Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin CN5258 - Asia - (PPE+PS)-X40 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin CN5258 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
NORYL™ CN5258 resin is a 40% filled blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This high modulus, injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VB at 2mm and V1 at 1.5mm. NORYL CN5258 resin exhibits good dimensional stability, low moisture absorption, high rigidity and is an excellent candidate for printer chassis applications.

UL Yellow Card Link E207780-228542
机械性能价值单位Test Standard
ASTM数据
弯曲模量 10000 MPa ASTM D 790
弯曲强度 158 MPa ASTM D 790
悬臂梁缺口冲击强度, 1/8 in 68 J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
1.5mm名义厚度时的燃烧性 V-1 class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
厚度为h时的5V燃烧性 5VB class IEC 60695-11-20
测试用试样的厚度 2.0 mm -
其它性能价值单位Test Standard
密度 1420 kg/m³ ASTM D 792
典型数据
加工方法
注塑
添加剂
阻燃剂
特殊性能
阻燃的
地区供应
亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com