Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer HPX4 - Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer HPX4 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable.

UL Yellow Card Link E207780-100566198
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 9 cm³/10min ISO 1133
温度 300 °C -
载荷 1.2 kg -
ASTM数据
熔融指数, MFI 10 g/10min ASTM D 1238
温度 300 °C -
负载 1.2 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2350 MPa ISO 527
屈服应力 57 MPa ISO 527
屈服伸长率 5.5 % ISO 527
断裂应力 61 MPa ISO 527
断裂伸长率 50 % ISO 527
弯曲模量 2150 MPa ISO 178
简支梁冲击强度, +23°C, 3mm N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C, 3mm N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C, 3mm 65 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C, 3mm 55 kJ/m² ISO 179/1eA
Izod冲击强度, +23°C N kJ/m² ISO 180/1U
悬臂梁缺口冲击强度, +23°C, 3mm 65 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度, -30°C, 3mm 55 kJ/m² ISO 180/1A
ASTM数据
拉伸模量 2210 MPa ASTM D 638
屈服应力 58 MPa ASTM D 638
断裂拉伸强度 64 MPa ASTM D 638
屈服伸长率 5.8 % ASTM D 638
断裂伸长率 131 % ASTM D 638
弯曲模量 2210 MPa ASTM D 790
洛克硬度 L89 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 890 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 795 J/m ASTM D 256
温度 -30 °C -
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 118 °C ISO 75-1/-2
维卡软化温度, B 141 °C ISO 306
维卡软化温度, 120°C/h 50N 142 °C ISO 306
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
厚度为h时的燃烧性 V-2 class IEC 60695-11-10
测试用试样的厚度 2.5 mm -
灼热丝燃烧指数 (GWFI) 960 °C IEC 60695-2-12
灼热丝引燃温度 (GWIT) 825 °C IEC 60695-2-13
GWIT - 测试用试样厚度 3 mm -
ASTM数据
DTUL @ 264 psi 124 °C ASTM D 648
维卡温度 141 °C ASTM D 1525
电性能价值单位Test Standard
ASTM数据
表面电阻率 1E15 Ohm ASTM D 257
体积电阻率 1E15 Ohm*cm ASTM D 257
其它性能价值单位Test Standard
吸水性 0.12 % 类似ISO 62
吸湿性 0.09 % 类似ISO 62
密度 1190 kg/m³ ISO 1183
密度 1190 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 120 °C -
预干燥-时间 3 - 4 h -
加工湿度 ≤0.02 % -
注塑熔体温度 295 - 315 °C -
模具温度 70 - 95 °C -
1区 270 - 295 °C -
2区 280 - 305 °C -
3区 295 - 315 °C -
螺杆转速 40 - 70 rpm -
背压 0.3 - 0.7 MPa -
典型数据
加工方法
注塑
特殊性能
环氧乙烷灭菌(EtO), 蒸汽灭菌, Gamma irradiation sterilization, Electron beam (e-beam) sterilization
Certifications
US药物六级认证
应用
药物
地区供应
亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.