Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer CXT17EX - Europe - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer CXT17EX - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
LEXAN™ CXT17EX resin is a High Heat Polycarbonate Copolymer Resin with Vicat of 170°C and crystal clear transparency. This resin is optimized for sheet and film extrusion applications, has a low plateout and a broad processing window with limited yellowing. It is available in limited transparent colors.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 27 cm³/10min ISO 1133
温度 330 °C -
载荷 2.16 kg -
ASTM数据
熔融指数, MFI 30 g/10min ASTM D 1238
温度 330 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2450 MPa ISO 527
屈服应力 75 MPa ISO 527
屈服伸长率 6.5 % ISO 527
断裂应力 60 MPa ISO 527
断裂伸长率 50 % ISO 527
弯曲模量 2500 MPa ISO 178
简支梁冲击强度, +23°C, 3mm N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C, 3mm 10 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C, 3mm 7 kJ/m² ISO 179/1eA
Izod冲击强度, +23°C N kJ/m² ISO 180/1U
悬臂梁缺口冲击强度, +23°C, 3mm 8 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度, -30°C, 3mm 7 kJ/m² ISO 180/1A
ASTM数据
拉伸模量 2500 MPa ASTM D 638
屈服应力 75 MPa ASTM D 638
断裂拉伸强度 60 MPa ASTM D 638
屈服伸长率 7 % ASTM D 638
断裂伸长率 40 % ASTM D 638
弯曲模量 2450 MPa ASTM D 790
悬臂梁缺口冲击强度, 1/8 in 80 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 75 J/m ASTM D 256
温度 -30 °C -
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 154 °C ISO 75-1/-2
热变形温度, 0.45 MPa 167 °C ISO 75-1/-2
维卡软化温度, 120°C/h 50N 174 °C ISO 306
热导率 0.2 W/(m K) DIN 52616
ASTM数据
DTUL @ 66 psi 167 °C ASTM D 648
DTUL @ 264 psi 154 °C ASTM D 648
其它性能价值单位Test Standard
吸水性 0.3 % 类似ISO 62
吸湿性 0.3 % 类似ISO 62
密度 1210 kg/m³ ISO 1183
密度 1210 kg/m³ ASTM D 792
典型数据
特殊性能
透明.
应用
汽车
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.