Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Desmopan 588 E - TPU - Covestro Deutschland AG

Material Data Center offers the following functions for Desmopan 588 E:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Desmopan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
  • Extrusion- and injection molding grade
  • improved microbial resistance
  • Improved hydrolysis resistance
    Application:
  • Cable sheathings
  • Hoses, non-reinforced
  • Roof lining
机械性能价值单位Test Standard
ISO数据
10%应变时的应力 1.8 MPa ISO 527
100%应变时的应力 5.9 MPa ISO 527
300%应变时的应力 10 MPa ISO 527
断裂应力 TPE 43 MPa ISO 527
断裂应变 TPE >300 % ISO 527
70°C时恒定应变下的永久变形, 24h 35 % ISO 815
撕裂强度 55 kN/m ISO 34-1
耐磨性 60 mm³ ISO 4649
肖氏硬度A 88 - ISO 7619-1
肖氏硬度D 33 - ISO 7619-1
其它性能价值单位Test Standard
密度 1150 kg/m³ ISO 1183
函数
动态剪切模量-温度 , Desmopan 588 E, TPU, Covestro
应力-应变(TPE) , Desmopan 588 E, TPU, Covestro
典型数据
加工方法
注塑, 异型材挤出成型, 片材挤出成型, 其它挤出成型, 表面涂层
供货形式
粒料
添加剂
润滑剂, 脱模助剂
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
PREPROCESSING
Max. water content: 0.05 %
Max. drying temperature: 80 °C
Drying time:
Dry air dryer 1-2 h

PROCESSING
Melt temperature: 210-230 °C
Mold temperature: 20-40 °C
其E烦龀尚
PROCESSING
Melt temperature: 190-210 °C
E尾募烦龀尚

 Preprocessing

Max. Water content ≤0.05 %
Drying temperature 70-110 °C
Dry air dryer 1-2 h
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.