Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Asaflex™ 825 - TPS - Asahi Kasei
Material Data Center offers the following functions for Asaflex™ 825:
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Asaflex datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
加工/物理特性 | 价值 | 单位 | Test Standard |
ISO数据 |
熔融指数, MFI |
6 |
g/10min |
ISO 1133 |
温度 |
200 |
°C |
- |
负载 |
5 |
kg |
- |
模塑收缩率, 平行 |
0.5 |
% |
ISO 294-4, 2577 |
机械性能 | 价值 | 单位 | Test Standard |
ISO数据 |
拉伸强度 |
27 |
MPa |
ISO 527 |
弯曲模量, 23°C |
1100 |
MPa |
ISO 178 |
弯曲强度 |
37 |
MPa |
ISO 178 |
简支梁冲击强度, +23°C |
100 |
kJ/m² |
ISO 179/1eU |
简支梁缺口冲击强度, +23°C |
2 |
kJ/m² |
ISO 179/1eA |
肖氏硬度D |
71 |
- |
ISO 7619-1 |
洛克硬度 |
R 55 |
- |
ISO 2039-2 |
热性能 | 价值 | 单位 | Test Standard |
ISO数据 |
热变形温度, 1.80 MPa |
57 |
°C |
ISO 75-1/-2 |
维卡软化温度, A |
76 |
°C |
ISO 306 |
光学特性 | 价值 | 单位 | Test Standard |
ISO Data |
浑浊率 |
0.5 |
- |
ISO 14782 |
Other Standards[S] |
光透射率 |
90 |
% |
ISO 13468 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
其它性能 | 价值 | 单位 | Test Standard |
吸水性 |
0.1 |
% |
类似ISO 62 |
密度 |
1020 |
kg/m³ |
ISO 1183 |
加工推荐(注塑) | 价值 | 单位 | Test Standard |
注塑熔体温度 |
180 - 220 |
°C |
- |
模具温度 |
50 |
°C |
- |
1区 |
180 - 200 |
°C |
- |
喷嘴温度 |
200 |
°C |
- |
注射压力 |
67 |
MPa |
- |
背压 |
6 |
MPa |
- |
加工推荐(挤出) | 价值 | 单位 | Test Standard |
模具温度 |
60 - 80 |
°C |
- |
1区 |
170 |
°C |
- |
2区 |
180 |
°C |
- |
3区 |
185 |
°C |
- |
4区 |
190 |
°C |
- |
5区 |
200 |
°C |
- |
喷嘴温度 |
200 |
°C |
- |
典型数据
加工方法
注塑, 其它挤出成型, 吹塑
特殊性能
高冲击韧性的/经抗冲改性的, 透明.
特征
High Gloss, 热稳定性, 共聚物
应用
包装
地区供应
北美, 欧洲, 亚太, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.