Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of ALFATER XL A90I 4FC0010 - TPV - MOCOM Compounds GmbH & Co. KG
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Alfater datasheets, application examples or technical articles are available in Material Data Center
材料类型 | PP/EPDM共混硫化热塑性弹性体 |
颜色 | 本色,固有颜色 |
工作温度 | 最大范围 (取决于负载,几何尺寸等) -40-125 °C |
主要特征 | 食品,konform EN 71-3,良好的染色性,良好的耐气候性,良好的抗化学性,耐臭氧,耐热空气,耐水解,高流动 |
市场分类 | 包装,家居用品,Lebensmittelindustrie,玩具 |
应用范围 | 注塑部件 |
主要应用 | 密封件,密封件,手柄,Soft-Touch Elemente,防护帽,盖子/容器,Behälter,Küchenwaren,2K-Bauteile |
机械性能 | 价值 | 单位 | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO数据 | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
撕裂强度 | 46 | kN/m | ISO 34-1 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
肖氏硬度A | 90 | - | ISO 7619-1 |
其它性能 | 价值 | 单位 | Test Standard |
密度 | 940 | kg/m³ | ISO 1183 |
烘干条件 | 在干燥空气(除湿)干燥器里 70-80 °C for 2-4 h 不必要的 <0,10 % |
注塑成型工艺 | 注塑熔体温度 195-230 °C 注塑模具温度 10-70 °C 中- 高注塑速度 >3 bar Nachdruck 50-70 % vom Spritzdruck |
储存 | 干燥,避免光照 fest verschlossen |