Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of ALFATER XL A85E 2GP0000 - TPV - MOCOM Compounds GmbH & Co. KG
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Alfater datasheets, application examples or technical articles are available in Material Data Center
材料类型 | PP/EPDM共混硫化热塑性弹性体 |
颜色 | 本色,黑色 |
工作温度 | 最大范围 (取决于负载,几何尺寸等) -40-125 °C |
主要特征 | 高粘度,良好的耐气候性,良好的抗化学性,耐臭氧,耐热空气,耐水解 |
市场分类 | 汽车,建筑,机械,电子电器,家具 |
应用范围 | 挤出部件,吹塑部件,Coextrusion |
主要应用 | 型材,密封件,密封件,导管,管路,线束导架,线缆护套,波纹管,空气导管,2K-Bauteile |
粘接于 | 均聚聚丙烯,Polypropylen Copolymer,聚乙烯,PP/EPDM共混硫化热塑性弹性体,烯烃类热塑性弹性体,常用热塑性弹性体 |
机械性能 | 价值 | 单位 | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO数据 | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
撕裂强度 | 50 | kN/m | ISO 34-1 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
肖氏硬度A | 85 | - | ISO 7619-1 |
其它性能 | 价值 | 单位 | Test Standard |
密度 | 940 | kg/m³ | ISO 1183 |
烘干条件 | 在干燥空气(除湿)干燥器里 70-80 °C for 2-4 h 不必要的 <0,10 % |
挤出成型工艺 | 注塑熔体温度 190-230 °C 模头温度 190-210 °C |
储存 | 干燥,避免光照 不高于30°C fest verschlossen |
烘干条件 | 在干燥空气(除湿)干燥器里 70-80 °C for 2-4 h 不必要的 <0,10 % |
挤出成型工艺 | 注塑熔体温度 190-230 °C 模头温度 190-210 °C |
储存 | 干燥,避免光照 不高于30°C tightly sealed |